Pb-free BGA solder joint reliability improvement with Sn3.5Ag solder alloy on Ni/Au finish
In this work, Sn3.5Ag solder alloy was being studied for the purpose of Pb-free solder joint reliability improvement over conventional Sn3.8Ag0.7Cu solder balls on Ball Grid Array (BGA) packages with Ni/Au pad finishing. The study was carried out in different levels. At individual solder joint level...
Saved in:
Main Authors: | Leng, E.P., Ding, M., Lindsay, W., Chopin, S., Ahmad, I., Jalar, A. |
---|---|
Format: | |
Published: |
2017
|
Online Access: | http://dspace.uniten.edu.my:8080/jspui/handle/123456789/5289 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
A comparative study of Sn3.5Ag and Sn3.8Ag0.7Cu for BGA spheres on Ni/Au finish
by: Eu, P.-L., et al.
Published: (2017) -
Investigation of Sn3.5Ag and Sn3.8Ag0.7Cu Pb-free Alloys for BGA application on Ni/Au Finish
by: Eu, P.-L., et al.
Published: (2017) -
Materials interaction during soldering and isothermal ageing of Sn-Pb and Sn-Ag-Cu solders on electroless Ni/Au surface finish
by: Tai, Siew Fong
Published: (2003) -
BGA lead-free C5 solder system improvement by germanium addition to Sn3.5Ag and Sn-3.8Ag-0.7Cu solder alloy
by: Leng, E.P., et al.
Published: (2017) -
A comparison study of SAC405 and SAC387 lead-free solder ball alloy characteristic and solder joint system on Ni/Au finish
by: Leng, E.P., et al.
Published: (2017)