Process optimization approach in fine pitch Cu wire bonding
With SiO2 dielectric under aluminum pads, a 60 m bond pad pitch with 52 um bond pad opening Cu wire bonding process was developed in PBGA Hip 7 PGE wafer technology. The critical factors (wire type, capillary, and bonding parameter) and critical responses (bonded ball diameter, bonded ball height, w...
Saved in:
Main Authors: | Wong B.K., Yong C.C., Eu P.L., Yap B.K. |
---|---|
Other Authors: | 36992192300 |
Format: | Conference paper |
Published: |
2023
|
Subjects: | |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Metallurgical bond integrity of C45 ultra fine pitch with 18m copper wire
by: Kid W.B., et al.
Published: (2023) -
Surface roughness and adhesion analysis study on ultrasonic gold ball onto aluminium bond pad
by: Vithyacharan, Retnasamy
Published: (2014) -
Wire bond shear test simulation on hemispherical surface bond pad
by: Zaliman, Sauli, Dr., et al.
Published: (2014) -
Characterization of Intermetallic Growth in Gold Ballbonds on Aluminum Metallization
by: Lim Moy Fung
Published: (2008) -
Ultra fine pitch Cu wire bonding on C45 ultra low k wafer technology
by: Leng E.P., et al.
Published: (2023)