Development and Working and Heat treatment strengthening of 2219 Aluminum alloy by mechanical working
The wrought aluminum alloy 2219 was developed using an induction furnace followed by forging and hot rolling for the improvement of properties. Then the alloy was solution treated at 535 ˚C for 48 minutes followed by water quenched and then aged at 210˚C, 230 ˚C and 240 ˚C for different time period....
Saved in:
Main Authors: | M. Rafi Raza, Rafi, Faiz Ahmad , Faiz, N.Ikram, Nazma, R.Ahmad, Rafiq, A.salam, Salam |
---|---|
Format: | Citation Index Journal |
Published: |
Asian Network for Scientific Information
2011
|
Subjects: | |
Online Access: | http://eprints.utp.edu.my/5141/1/2219_Al__alloy_%28JAS2011%29.ppt.pdf http://eprints.utp.edu.my/5141/ |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Nanomechanical, mechanical and microstructural characterization of electron beam welded Al2219-T6 tempered aerospace grade alloy: A comprehensive study
by: Hussain, Ghulam, et al.
Published: (2024) -
Influence of heat treatment on the microstructure and mechanical properties of 6061 aluminum alloy
by: Luqman Nulhaqem, Abdul Aziz
Published: (2013) -
Influence Of Short Heat Treatment On The Microstructures And Mechanical Properties Of Thixoformed Aluminum Alloy Composite
by: Salleh, Mohd Shukor, et al.
Published: (2021) -
Precipitation strengthening in extruded AZ61 magnesium alloys during heat treatment process
by: Mohd Daud, Mohd Ahadlin, et al.
Published: (2013) -
Precipitation strengthening in extruded AZ61 magnesium alloys during heat treatment process
by: Mohd Daud, Mohd Ahadlin, et al.
Published: (2013)