The wrought aluminum alloy 2219 was developed using an induction furnace followed by forging and hot rolling for the improvement of properties. Then the alloy was solution treated at 535 ˚C for 48 minutes followed by water quenched and then aged at 210˚C, 230 ˚C and 240 ˚C for different time period....