Structural Integrity Study Of Ultra-Fine Solder Joint Using Microscopy Investigation
The electronic industries are changing the solder used from the lead solder to the lead-free solder. The elimination of lead solder is done due to the new laws and restrictions. The lead-free solder is extensively used in the electronic assemblies and there is also concerns about the lead-free solde...
Saved in:
Main Author: | |
---|---|
Format: | Monograph |
Language: | English |
Published: |
Universiti Sains Malaysia
2017
|
Subjects: | |
Online Access: | http://eprints.usm.my/54408/1/Structural%20Integrity%20Study%20Of%20Ultra-Fine%20Solder%20Joint%20Using%20Microscopy%20Investigation_Mohd%20Amier%20Hasief%20%20Mat%20Zahit_M4_2017.pdf http://eprints.usm.my/54408/ |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
id |
my.usm.eprints.54408 |
---|---|
record_format |
eprints |
spelling |
my.usm.eprints.54408 http://eprints.usm.my/54408/ Structural Integrity Study Of Ultra-Fine Solder Joint Using Microscopy Investigation Zahit, Mohd Amier Hasief Mat T Technology TJ1 Mechanical engineering and machinery The electronic industries are changing the solder used from the lead solder to the lead-free solder. The elimination of lead solder is done due to the new laws and restrictions. The lead-free solder is extensively used in the electronic assemblies and there is also concerns about the lead-free solder reliability. Solder joints in electronic products are used as interconnection material for enabling electrical, thermal and mechanical function in the electronic packaging. Addition of nano particles in the solder joint is to investigate the relation between the percentage and the quality of the solder joint. The quality of the solder joints is one of the most important aspect that we need to consider to make a good solder joint. The hardness test of the solder joint is to know what is the relation between hardness and the percentage of the nano particles in solder joint. Three types of solder joints that contain 0.01%, 0.05%, and 0.15% of Fe2O3 (Feric Oxide) are used in the experiment with small (01005), medium (0603) and big (0805) size of the component. Universiti Sains Malaysia 2017-06-01 Monograph NonPeerReviewed application/pdf en http://eprints.usm.my/54408/1/Structural%20Integrity%20Study%20Of%20Ultra-Fine%20Solder%20Joint%20Using%20Microscopy%20Investigation_Mohd%20Amier%20Hasief%20%20Mat%20Zahit_M4_2017.pdf Zahit, Mohd Amier Hasief Mat (2017) Structural Integrity Study Of Ultra-Fine Solder Joint Using Microscopy Investigation. Project Report. Universiti Sains Malaysia, Pusat Pengajian Kejuruteraan Mekanik. (Submitted) |
institution |
Universiti Sains Malaysia |
building |
Hamzah Sendut Library |
collection |
Institutional Repository |
continent |
Asia |
country |
Malaysia |
content_provider |
Universiti Sains Malaysia |
content_source |
USM Institutional Repository |
url_provider |
http://eprints.usm.my/ |
language |
English |
topic |
T Technology TJ1 Mechanical engineering and machinery |
spellingShingle |
T Technology TJ1 Mechanical engineering and machinery Zahit, Mohd Amier Hasief Mat Structural Integrity Study Of Ultra-Fine Solder Joint Using Microscopy Investigation |
description |
The electronic industries are changing the solder used from the lead solder to the lead-free solder. The elimination of lead solder is done due to the new laws and restrictions. The lead-free solder is extensively used in the electronic assemblies and there is also concerns about the lead-free solder reliability. Solder joints in electronic products are used as interconnection material for enabling electrical, thermal and mechanical function in the electronic packaging. Addition of nano particles in the solder joint is to investigate the relation between the percentage and the quality of the solder joint. The quality of the solder joints is one of the most important aspect that we need to consider to make a good solder joint. The hardness test of the solder joint is to know what is the relation between hardness and the percentage of the nano particles in solder joint. Three types of solder joints that contain 0.01%, 0.05%, and 0.15% of Fe2O3 (Feric Oxide) are used in the experiment with small (01005), medium (0603) and big (0805) size of the component. |
format |
Monograph |
author |
Zahit, Mohd Amier Hasief Mat |
author_facet |
Zahit, Mohd Amier Hasief Mat |
author_sort |
Zahit, Mohd Amier Hasief Mat |
title |
Structural Integrity Study Of Ultra-Fine Solder Joint Using Microscopy Investigation |
title_short |
Structural Integrity Study Of Ultra-Fine Solder Joint Using Microscopy Investigation |
title_full |
Structural Integrity Study Of Ultra-Fine Solder Joint Using Microscopy Investigation |
title_fullStr |
Structural Integrity Study Of Ultra-Fine Solder Joint Using Microscopy Investigation |
title_full_unstemmed |
Structural Integrity Study Of Ultra-Fine Solder Joint Using Microscopy Investigation |
title_sort |
structural integrity study of ultra-fine solder joint using microscopy investigation |
publisher |
Universiti Sains Malaysia |
publishDate |
2017 |
url |
http://eprints.usm.my/54408/1/Structural%20Integrity%20Study%20Of%20Ultra-Fine%20Solder%20Joint%20Using%20Microscopy%20Investigation_Mohd%20Amier%20Hasief%20%20Mat%20Zahit_M4_2017.pdf http://eprints.usm.my/54408/ |
_version_ |
1743107826298912768 |
score |
13.214268 |