A study of the kinetics and mechanism of the adsorption and anaerobic partial oxidation of n-butane over a vanadyl pyrophosphate catalyst

The interaction of n-butane with a ((VO)2P2O7) catalyst has been investigated by temperature-programmed desorption and anaerobic temperature-programmed reaction. n-Butane has been shown to adsorb on the (VO)2P2O7 to as a butyl–hydroxyl pair. When adsorption is carried out at 223 K, upon temperature...

Full description

Saved in:
Bibliographic Details
Main Authors: Sakakini, Bahij H., Yap, Taufiq Yun Hin, Waugh, Kenneth Charles
Format: Article
Language:English
English
Published: Elsevier 2000
Online Access:http://psasir.upm.edu.my/id/eprint/7881/1/A%20study%20of%20the%20kinetics%20and%20mechanism%20of%20the%20adsorption%20and%20anaerobic%20partial%20oxidation%20of%20n-butane%20over%20a%20vanadyl%20pyrophosphate%20catalyst.pdf
http://psasir.upm.edu.my/id/eprint/7881/7/1-s2.0-S0021951799925137-main.pdf
http://psasir.upm.edu.my/id/eprint/7881/
http://dx.doi.org/10.1006/jcat.1999.2513
Tags: Add Tag
No Tags, Be the first to tag this record!
id my.upm.eprints.7881
record_format eprints
spelling my.upm.eprints.78812024-08-05T06:51:21Z http://psasir.upm.edu.my/id/eprint/7881/ A study of the kinetics and mechanism of the adsorption and anaerobic partial oxidation of n-butane over a vanadyl pyrophosphate catalyst Sakakini, Bahij H. Yap, Taufiq Yun Hin Waugh, Kenneth Charles The interaction of n-butane with a ((VO)2P2O7) catalyst has been investigated by temperature-programmed desorption and anaerobic temperature-programmed reaction. n-Butane has been shown to adsorb on the (VO)2P2O7 to as a butyl–hydroxyl pair. When adsorption is carried out at 223 K, upon temperature programming some of the butyl–hydroxyl species recombine resulting in butane desorption at 260 K. However, when adsorption is carried out at 423 K, the hydroxyl species of the butyl–hydroxyl pair migrate away from the butyl species during the adsorption, forming water which is detected in the gas phase. Butane therefore is not observed to desorb at 260 K after we lowered the temperature to 223 K under the butane/helium from the adsorption temperature of 423 K prior to temperature programming from that temperature to 1100 K under a helium stream. Anaerobic temperature-programmed oxidation of n-butane produces butene and butadiene at a peak maximum temperature of 1000 K; this is exactly the temperature at which, upon temperature programming, oxygen evolves from the lattice and desorbs as O2. This, and the fact that the amount of oxygen desorbing from the (VO)2P2O7 at 1000 K is the same as that required for the oxidation of the n-butane to butene and butadiene, strongly suggests (i) that lattice oxygen as it emerges at the surface is the selective oxidant and (ii) that its appearance at the surface is the rate-determining step in the selective oxidation of n-butane. The surface of the (VO)2P2O7 catalyst on which this selective oxidation takes place has had approximately two monolayers of oxygen removed from it by unselective oxidation of the n-butane to CO, CO2, and H2O between 550 and 950 K and has had approximately one monolayer of carbon deposited on it at 1000 K. It is apparent, therefore, that the original crystallography of the (VO)2P2O7 catalyst will not exist during this selective oxidation and that theories that relate selectivity in partial oxidation to the (100) face of the (VO)2P2O7 catalyst cannot apply in this case. Elsevier 2000-01-25 Article PeerReviewed text en http://psasir.upm.edu.my/id/eprint/7881/1/A%20study%20of%20the%20kinetics%20and%20mechanism%20of%20the%20adsorption%20and%20anaerobic%20partial%20oxidation%20of%20n-butane%20over%20a%20vanadyl%20pyrophosphate%20catalyst.pdf text en http://psasir.upm.edu.my/id/eprint/7881/7/1-s2.0-S0021951799925137-main.pdf Sakakini, Bahij H. and Yap, Taufiq Yun Hin and Waugh, Kenneth Charles (2000) A study of the kinetics and mechanism of the adsorption and anaerobic partial oxidation of n-butane over a vanadyl pyrophosphate catalyst. Journal of Catalysis, 189 (2). pp. 253-262. ISSN 0021-9517 http://dx.doi.org/10.1006/jcat.1999.2513 10.1006/jcat.1999.2513
institution Universiti Putra Malaysia
building UPM Library
collection Institutional Repository
continent Asia
country Malaysia
content_provider Universiti Putra Malaysia
content_source UPM Institutional Repository
url_provider http://psasir.upm.edu.my/
language English
English
description The interaction of n-butane with a ((VO)2P2O7) catalyst has been investigated by temperature-programmed desorption and anaerobic temperature-programmed reaction. n-Butane has been shown to adsorb on the (VO)2P2O7 to as a butyl–hydroxyl pair. When adsorption is carried out at 223 K, upon temperature programming some of the butyl–hydroxyl species recombine resulting in butane desorption at 260 K. However, when adsorption is carried out at 423 K, the hydroxyl species of the butyl–hydroxyl pair migrate away from the butyl species during the adsorption, forming water which is detected in the gas phase. Butane therefore is not observed to desorb at 260 K after we lowered the temperature to 223 K under the butane/helium from the adsorption temperature of 423 K prior to temperature programming from that temperature to 1100 K under a helium stream. Anaerobic temperature-programmed oxidation of n-butane produces butene and butadiene at a peak maximum temperature of 1000 K; this is exactly the temperature at which, upon temperature programming, oxygen evolves from the lattice and desorbs as O2. This, and the fact that the amount of oxygen desorbing from the (VO)2P2O7 at 1000 K is the same as that required for the oxidation of the n-butane to butene and butadiene, strongly suggests (i) that lattice oxygen as it emerges at the surface is the selective oxidant and (ii) that its appearance at the surface is the rate-determining step in the selective oxidation of n-butane. The surface of the (VO)2P2O7 catalyst on which this selective oxidation takes place has had approximately two monolayers of oxygen removed from it by unselective oxidation of the n-butane to CO, CO2, and H2O between 550 and 950 K and has had approximately one monolayer of carbon deposited on it at 1000 K. It is apparent, therefore, that the original crystallography of the (VO)2P2O7 catalyst will not exist during this selective oxidation and that theories that relate selectivity in partial oxidation to the (100) face of the (VO)2P2O7 catalyst cannot apply in this case.
format Article
author Sakakini, Bahij H.
Yap, Taufiq Yun Hin
Waugh, Kenneth Charles
spellingShingle Sakakini, Bahij H.
Yap, Taufiq Yun Hin
Waugh, Kenneth Charles
A study of the kinetics and mechanism of the adsorption and anaerobic partial oxidation of n-butane over a vanadyl pyrophosphate catalyst
author_facet Sakakini, Bahij H.
Yap, Taufiq Yun Hin
Waugh, Kenneth Charles
author_sort Sakakini, Bahij H.
title A study of the kinetics and mechanism of the adsorption and anaerobic partial oxidation of n-butane over a vanadyl pyrophosphate catalyst
title_short A study of the kinetics and mechanism of the adsorption and anaerobic partial oxidation of n-butane over a vanadyl pyrophosphate catalyst
title_full A study of the kinetics and mechanism of the adsorption and anaerobic partial oxidation of n-butane over a vanadyl pyrophosphate catalyst
title_fullStr A study of the kinetics and mechanism of the adsorption and anaerobic partial oxidation of n-butane over a vanadyl pyrophosphate catalyst
title_full_unstemmed A study of the kinetics and mechanism of the adsorption and anaerobic partial oxidation of n-butane over a vanadyl pyrophosphate catalyst
title_sort study of the kinetics and mechanism of the adsorption and anaerobic partial oxidation of n-butane over a vanadyl pyrophosphate catalyst
publisher Elsevier
publishDate 2000
url http://psasir.upm.edu.my/id/eprint/7881/1/A%20study%20of%20the%20kinetics%20and%20mechanism%20of%20the%20adsorption%20and%20anaerobic%20partial%20oxidation%20of%20n-butane%20over%20a%20vanadyl%20pyrophosphate%20catalyst.pdf
http://psasir.upm.edu.my/id/eprint/7881/7/1-s2.0-S0021951799925137-main.pdf
http://psasir.upm.edu.my/id/eprint/7881/
http://dx.doi.org/10.1006/jcat.1999.2513
_version_ 1806690475018551296
score 13.214268