Investigation on wall thinning and creep damage in boiler tube due to scale formation
Boiler is a closed vessel in which the water is heated up to convert it from the liquid phase to superheat steam at specified pressure by addition of heat. The tubes are operated continuously at high temperature due to the formation of scale which has lower conductivity than that of steel. The scale...
محفوظ في:
المؤلفون الرئيسيون: | Begum S., Mustafizul Karim A.N., Shafii M.A. |
---|---|
مؤلفون آخرون: | 7101852571 |
التنسيق: | Conference paper |
منشور في: |
2023
|
الموضوعات: | |
الوسوم: |
إضافة وسم
لا توجد وسوم, كن أول من يضع وسما على هذه التسجيلة!
|
مواد مشابهة
-
Failure case studies of SA213-T22 steel tubes of boiler through computer simulations
بواسطة: Purbolaksono J., وآخرون
منشور في: (2023) -
Failure investigation on reheater tube due to deposit and wall thinning
بواسطة: Purbolaksono J., وآخرون
منشور في: (2023) -
Mechanichal Porperies of Boiler Tubes ( T91 AND T92)
بواسطة: Kalairasan A /l Anparassan
منشور في: (2023) -
Thermal fatigue and corrosion fatigue in heat recovery area wall side tubes
بواسطة: Ahmad J., وآخرون
منشور في: (2023) -
Failure investigation on rear water wall tube of boiler
بواسطة: Ahmad J., وآخرون
منشور في: (2023)