Electrical properties and microstructure of magnetoresistive (La1-xSrxMnO3(x = 0.0, 0.05, 0.15 and 0.3)
The insulator-metal transition temperature, Tim of Lal-x SrxMnO3 (x = 0.0, 0-05, 0.15 and 0.3) was studied during warming and cooling between 50 K to 300 K. The results showed that Tim of Lal-x SrxMnO3 shifted to a higher temperature as Sr was substituted for La. Scanning electron micrographs showed...
Saved in:
Main Authors: | , , |
---|---|
Other Authors: | |
Format: | Article |
Published: |
2023
|
Subjects: | |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
id |
my.uniten.dspace-29791 |
---|---|
record_format |
dspace |
spelling |
my.uniten.dspace-297912023-12-28T16:57:41Z Electrical properties and microstructure of magnetoresistive (La1-xSrxMnO3(x = 0.0, 0.05, 0.15 and 0.3) Ewe L.S. Hamid N.A. Abd-Shukor R. 58032789200 6604077116 7004750914 Electrical resistance Magnetoresistance Microstructure The insulator-metal transition temperature, Tim of Lal-x SrxMnO3 (x = 0.0, 0-05, 0.15 and 0.3) was studied during warming and cooling between 50 K to 300 K. The results showed that Tim of Lal-x SrxMnO3 shifted to a higher temperature as Sr was substituted for La. Scanning electron micrographs showed that the average grain size is in the range of 0.6 ?m - 1.4 ?m. Grain boundaries are almost completely revealed for x = 0.3. X-Ray powder diffraction patterns showed cubic structure (space group Pm-3m) and contain no secondary phases. Final 2023-12-28T08:57:41Z 2023-12-28T08:57:41Z 2006 Article 2-s2.0-34548743934 https://www.scopus.com/inward/record.uri?eid=2-s2.0-34548743934&partnerID=40&md5=30486116338cb9c7cfa6919bc1953cab https://irepository.uniten.edu.my/handle/123456789/29791 35 2 73 77 Scopus |
institution |
Universiti Tenaga Nasional |
building |
UNITEN Library |
collection |
Institutional Repository |
continent |
Asia |
country |
Malaysia |
content_provider |
Universiti Tenaga Nasional |
content_source |
UNITEN Institutional Repository |
url_provider |
http://dspace.uniten.edu.my/ |
topic |
Electrical resistance Magnetoresistance Microstructure |
spellingShingle |
Electrical resistance Magnetoresistance Microstructure Ewe L.S. Hamid N.A. Abd-Shukor R. Electrical properties and microstructure of magnetoresistive (La1-xSrxMnO3(x = 0.0, 0.05, 0.15 and 0.3) |
description |
The insulator-metal transition temperature, Tim of Lal-x SrxMnO3 (x = 0.0, 0-05, 0.15 and 0.3) was studied during warming and cooling between 50 K to 300 K. The results showed that Tim of Lal-x SrxMnO3 shifted to a higher temperature as Sr was substituted for La. Scanning electron micrographs showed that the average grain size is in the range of 0.6 ?m - 1.4 ?m. Grain boundaries are almost completely revealed for x = 0.3. X-Ray powder diffraction patterns showed cubic structure (space group Pm-3m) and contain no secondary phases. |
author2 |
58032789200 |
author_facet |
58032789200 Ewe L.S. Hamid N.A. Abd-Shukor R. |
format |
Article |
author |
Ewe L.S. Hamid N.A. Abd-Shukor R. |
author_sort |
Ewe L.S. |
title |
Electrical properties and microstructure of magnetoresistive (La1-xSrxMnO3(x = 0.0, 0.05, 0.15 and 0.3) |
title_short |
Electrical properties and microstructure of magnetoresistive (La1-xSrxMnO3(x = 0.0, 0.05, 0.15 and 0.3) |
title_full |
Electrical properties and microstructure of magnetoresistive (La1-xSrxMnO3(x = 0.0, 0.05, 0.15 and 0.3) |
title_fullStr |
Electrical properties and microstructure of magnetoresistive (La1-xSrxMnO3(x = 0.0, 0.05, 0.15 and 0.3) |
title_full_unstemmed |
Electrical properties and microstructure of magnetoresistive (La1-xSrxMnO3(x = 0.0, 0.05, 0.15 and 0.3) |
title_sort |
electrical properties and microstructure of magnetoresistive (la1-xsrxmno3(x = 0.0, 0.05, 0.15 and 0.3) |
publishDate |
2023 |
_version_ |
1806423241296707584 |
score |
13.214268 |