Electrical properties and microstructure of magnetoresistive (La1-xSrxMnO3(x = 0.0, 0.05, 0.15 and 0.3)
The insulator-metal transition temperature, Tim of Lal-x SrxMnO3 (x = 0.0, 0-05, 0.15 and 0.3) was studied during warming and cooling between 50 K to 300 K. The results showed that Tim of Lal-x SrxMnO3 shifted to a higher temperature as Sr was substituted for La. Scanning electron micrographs showed...
Saved in:
Main Authors: | Ewe L.S., Hamid N.A., Abd-Shukor R. |
---|---|
Other Authors: | 58032789200 |
Format: | Article |
Published: |
2023
|
Subjects: | |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Elastic moduli and sound velocity in La1-xSrxMnO 3 (x = 0 to 0.3)
by: Ewe L.S., et al.
Published: (2023) -
Electrical properties and microstructure of magnetoresistive
( (x = 0.0, 0.05, 0.15 and 0.3)
by: Ewe, L.S., et al.
Published: (2006) -
Structural and microstructure of magnetoresistive ND1-XBAXMNO3 (X=0.2, 0.25, 0.3 and 0.35)
by: Tan Jong Jee
Published: (2023) -
Electrical transport properties of Pr1-xSrxMnO 3 (x = 0 to 0�45)
by: Ewe L.S., et al.
Published: (2023) -
Colossal magnetoresistance of La0.67Ca0.33Mn1-xAx)3 [A=V, Dy and Zr] perovskite
by: Koh, Song Foo
Published: (2001)