Fe-Al Diffusion Bonding: Effect of reaction time on the interlayer thickness / Asmawi Ismail...[et al.]
A direct diffusion bonding of marine grade aluminium alloy AA6061 and steel A36 was carried out in an argon environment at 640°C. Specimens were heated in a furnace for a holding time of 90 to 120 min under a pre-pressed condition. An interface microstructural observation revealed an increase in the...
Saved in:
Main Authors: | Ismail, Asmawi, Hussain, Patthi, Mustapha, Mazli, Nuruddin, Muhd Fadhil |
---|---|
Format: | Article |
Language: | English |
Published: |
Faculty of Mechanical Engineering Universiti Teknologi MARA (UiTM)
2018
|
Subjects: | |
Online Access: | http://ir.uitm.edu.my/id/eprint/36294/1/36294.pdf http://ir.uitm.edu.my/id/eprint/36294/ https://jmeche.uitm.edu.my/ |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Optimisation of Fe-Al Diffusion Bonding in Air
by: Ismail, A., et al.
Published: (2023) -
Mechanical performance and corrosion behaviour of diffusion-bonded A5083 aluminium and A36 mild steel with gallium interlayer
by: Ismail, Asmawi, et al.
Published: (2022) -
Bearing damage analysis / Md. Asmawi Said and Wan Sadeli Wan Ismail
by: Said, Md. Asmawi, et al.
Published: (2001) -
Watson Kota Bharu / Muhammad Haikal Mohd Asmawi
by: Mohd Asmawi, Muhammad Haikal
Published: (2021) -
Business Opportunity: Card Capital / Muhammad Haikal Mohd Asmawi
by: Mohd Asmawi, Muhammad Haikal
Published: (2021)