Surface hardness of friction stir welded AA6063 pipe
The external surface hardness of friction stir welded aluminum alloy 6063 pipe joint was investigated in this paper. The 89mm of outside diameter pipe with 5mm of wall thickness was used as test pipe piece for this experiment on closed butt joint configuration by utilising Bridgeport 2216 CNC millin...
Saved in:
Main Authors: | Ismail, A., Awang, M. |
---|---|
Format: | Conference or Workshop Item |
Published: |
EDP Sciences
2014
|
Online Access: | https://www.scopus.com/inward/record.uri?eid=2-s2.0-84904991941&doi=10.1051%2fmatecconf%2f20141304025&partnerID=40&md5=e9b4f01ff79bd80bb3e979b13f9e6232 http://eprints.utp.edu.my/32261/ |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Evaluation of the hardness distribution and fracture location in friction stir welded AA6063 pipe butt joints
by: Ismail, A., et al.
Published: (2018) -
Evaluation of the hardness distribution and fracture location in friction stir welded AA6063 pipe butt joints
by: Ismail, A., et al.
Published: (2018) -
INFLUENCE OF FRICTION STIR WELDING
PARAMETERS ON THE MECHANICAL PROPERTIES OF AA6063 PIPE BUTT
by: ISMAIL, AZMAN
Published: (2020) -
Optimization of Welding Parameters for Self-Support Friction Stir Welding (SS-FSW) on AA6063 Pipe Joints
by: Lotpy, M.A.M.N., et al.
Published: (2021) -
Temperature profile and fracture location of friction stir welded AA6063-T6 pipe butt joint
by: Ismail, A., et al.
Published: (2016)