Development of magnetic graphene oxide adsorbent for the removal and preconcentration of As(III) and As(V) species from environmental water samples

New-generation adsorbent, Fe3O4@SiO2/GO, was developed by modification of graphene oxide (GO) with silica-coated (SiO2) magnetic nanoparticles (Fe3O4). The synthesized adsorbent was characterized using Fourier transform infrared spectroscopy, X-ray diffractometry, energy-dispersive X-ray spectroscop...

Full description

Saved in:
Bibliographic Details
Main Authors: Nodeh, Hamid Rashidi, Wan Ibrahim, Wan Aini, Ali, Imran, Mohd. Marsin, Sanagi
Format: Article
Published: Springer-Verlag 2016
Subjects:
Online Access:http://eprints.utm.my/id/eprint/69199/
http://dx.doi.org/10.1007/s11356-016-6137-z
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:New-generation adsorbent, Fe3O4@SiO2/GO, was developed by modification of graphene oxide (GO) with silica-coated (SiO2) magnetic nanoparticles (Fe3O4). The synthesized adsorbent was characterized using Fourier transform infrared spectroscopy, X-ray diffractometry, energy-dispersive X-ray spectroscopy, and field emission scanning electron microscopy. The developed adsorbent was used for the removal and simultaneous preconcentration of As(III) and As(V) from environmental waters prior to ICP-MS analysis. Fe3O4@SiO2/GO provided high adsorption capacities, i.e., 7.51 and 11.46 mg g−1 for As(III) and As(V), respectively, at pH 4.0. Adsorption isotherm, kinetic, and thermodynamic were investigated for As(III) and As(V) adsorption. Preconcentration of As(III) and As(V) were studied using magnetic solid-phase extraction (MSPE) method at pH 9.0 as the adsorbent showed selective adsorption for As(III) only in pH range 7–10. MSPE using Fe3O4@SiO2/GO was developed with good linearities (0.05–2.0 ng mL−1) and high coefficient of determination (R2 = 0.9992 and 0.9985) for As(III) and As(V), respectively. The limits of detection (LODs) (3× SD/m, n = 3) obtained were 7.9 pg mL−1 for As(III) and 28.0 pg mL−1 for As(V). The LOD obtained is 357–1265× lower than the WHO maximum permissible limit of 10.0 ng mL−1. The developed MSPE method showed good relative recoveries (72.55–109.71 %) and good RSDs (0.1–4.3 %, n = 3) for spring water, lake, river, and tap water samples. The new-generation adsorbent can be used for the removal and simultaneous preconcentration of As(III) and As(V) from water samples successfully. The adsorbent removal for As(III) is better than As(V).