The influence of SS316l foam fabrication parameter using powder metallurgy route

Metal foams are widely produced by using different techniques such as compaction and replication method. In this study, slurry method also known as replication method has been used to produce SS316L foams. SS316L powders (50wt% and 60wt%) were mixed with the binders and distilled water by using mech...

Full description

Saved in:
Bibliographic Details
Main Authors: Mad Rosip, N. I., Ahmad, Sufizar, Jamaluddin, Khairur Rijal, Mat Nor, F.
Format: Conference or Workshop Item
Published: 2014
Subjects:
Online Access:http://eprints.utm.my/id/eprint/68568/
http://www.ttp.net/978-3-03835-149-8.html
Tags: Add Tag
No Tags, Be the first to tag this record!
id my.utm.68568
record_format eprints
spelling my.utm.685682017-10-08T03:31:22Z http://eprints.utm.my/id/eprint/68568/ The influence of SS316l foam fabrication parameter using powder metallurgy route Mad Rosip, N. I. Ahmad, Sufizar Jamaluddin, Khairur Rijal Mat Nor, F. T Technology (General) Metal foams are widely produced by using different techniques such as compaction and replication method. In this study, slurry method also known as replication method has been used to produce SS316L foams. SS316L powders (50wt% and 60wt%) were mixed with the binders and distilled water by using mechanical stirrer. Polyethylene Glycol (PEG) and Carboxyl Methyl Cellulose (CMC) were used as binders. Polyurethane (PU) foam was used as scaffold and dipped into SS316L slurry then dried in room temperature for 24 hours. Sintering process has been done in two different temperatures which were 1200oC and 1300oC in vacuum furnace. The morphological study was performed using Scanning Electron Microscopy (SEM) and Energy Dispersive X-Ray (EDX). The SEM micrograph showed that the cells were interconnected and the structures become denser as the sintering temperature increase. The average pores size is ranging from 252.8 μm-353.8 μm, while strut size ranging from 50.2 μm -79.9 μm based on SEM micrograph analysis. The elemental analysis from EDX showed the element presence in the SS316L foam remain from SS316L powder which are Chromium (Cr), Nickel (Ni), Molybdenum (Mo), Cooper (Cu), Nitrogen (N2), Sulphur (S) and Silicon (Si). Higher sintering temperature contributes better grain growth between particles where the point-contact between the particles expanded and disappear the small pores. 2014 Conference or Workshop Item PeerReviewed Mad Rosip, N. I. and Ahmad, Sufizar and Jamaluddin, Khairur Rijal and Mat Nor, F. (2014) The influence of SS316l foam fabrication parameter using powder metallurgy route. In: 5th International Conference on Material and Manufacturing Technology, ICMMT 2014, 8-9 May, 2014, Kuala Lumpur, Malaysia. http://www.ttp.net/978-3-03835-149-8.html
institution Universiti Teknologi Malaysia
building UTM Library
collection Institutional Repository
continent Asia
country Malaysia
content_provider Universiti Teknologi Malaysia
content_source UTM Institutional Repository
url_provider http://eprints.utm.my/
topic T Technology (General)
spellingShingle T Technology (General)
Mad Rosip, N. I.
Ahmad, Sufizar
Jamaluddin, Khairur Rijal
Mat Nor, F.
The influence of SS316l foam fabrication parameter using powder metallurgy route
description Metal foams are widely produced by using different techniques such as compaction and replication method. In this study, slurry method also known as replication method has been used to produce SS316L foams. SS316L powders (50wt% and 60wt%) were mixed with the binders and distilled water by using mechanical stirrer. Polyethylene Glycol (PEG) and Carboxyl Methyl Cellulose (CMC) were used as binders. Polyurethane (PU) foam was used as scaffold and dipped into SS316L slurry then dried in room temperature for 24 hours. Sintering process has been done in two different temperatures which were 1200oC and 1300oC in vacuum furnace. The morphological study was performed using Scanning Electron Microscopy (SEM) and Energy Dispersive X-Ray (EDX). The SEM micrograph showed that the cells were interconnected and the structures become denser as the sintering temperature increase. The average pores size is ranging from 252.8 μm-353.8 μm, while strut size ranging from 50.2 μm -79.9 μm based on SEM micrograph analysis. The elemental analysis from EDX showed the element presence in the SS316L foam remain from SS316L powder which are Chromium (Cr), Nickel (Ni), Molybdenum (Mo), Cooper (Cu), Nitrogen (N2), Sulphur (S) and Silicon (Si). Higher sintering temperature contributes better grain growth between particles where the point-contact between the particles expanded and disappear the small pores.
format Conference or Workshop Item
author Mad Rosip, N. I.
Ahmad, Sufizar
Jamaluddin, Khairur Rijal
Mat Nor, F.
author_facet Mad Rosip, N. I.
Ahmad, Sufizar
Jamaluddin, Khairur Rijal
Mat Nor, F.
author_sort Mad Rosip, N. I.
title The influence of SS316l foam fabrication parameter using powder metallurgy route
title_short The influence of SS316l foam fabrication parameter using powder metallurgy route
title_full The influence of SS316l foam fabrication parameter using powder metallurgy route
title_fullStr The influence of SS316l foam fabrication parameter using powder metallurgy route
title_full_unstemmed The influence of SS316l foam fabrication parameter using powder metallurgy route
title_sort influence of ss316l foam fabrication parameter using powder metallurgy route
publishDate 2014
url http://eprints.utm.my/id/eprint/68568/
http://www.ttp.net/978-3-03835-149-8.html
_version_ 1643655961538199552
score 13.160551