Characterisation of calcium phosphate coating on investment cast 316L stainless steel
Medical grade 316L stainless steel (316L-SS) was coated with hydroxyapatite (HA) using investment casting technique. The molten metal was poured into a HA coated ceramic mould at 1650°C under vacuum. The coated samples were vacuum sintered in a furnace at three different temperatures for 1 h. The ca...