Effect of oil palm fibre addition on the mechanical properties of shell mould investment casting

This research is aimed to investigate the effect of addition of organic fibre on the mechanical properties of the investment casting ceramic mould based on different length of fibres in the investment. Modulus of rupture (MOR) and permeability of the ceramic mould are evaluated. The MOR test contain...

Full description

Saved in:
Bibliographic Details
Main Author: Soh, Wen Hann
Format: Thesis
Language:English
Published: 2009
Subjects:
Online Access:http://eprints.utm.my/id/eprint/12221/6/SohWenHannMFKM2009.pdf
http://eprints.utm.my/id/eprint/12221/
Tags: Add Tag
No Tags, Be the first to tag this record!
id my.utm.12221
record_format eprints
spelling my.utm.122212017-09-14T00:23:15Z http://eprints.utm.my/id/eprint/12221/ Effect of oil palm fibre addition on the mechanical properties of shell mould investment casting Soh, Wen Hann TJ Mechanical engineering and machinery TS Manufactures This research is aimed to investigate the effect of addition of organic fibre on the mechanical properties of the investment casting ceramic mould based on different length of fibres in the investment. Modulus of rupture (MOR) and permeability of the ceramic mould are evaluated. The MOR test contains three systems: green (undewaxed), green (dewaxed) and fired. The permeability test contains two systems: green (dewaxed) and fired. For the variation of fibre length, 3mm, 5mm, 7mm, 9mm are established. In each system, the MOR and permeability are compared between the fibre addition specimens and the non fibre addition specimen. Oil palm empty fruit bunch fibre is used as the additive in the investments. Colloidal silica and zircon sand are used to produce the ceramic mould. Firing temperature used is 700ºC. MOR three point bending testing machine is used to evaluate the strength of the mould. Permeability tester is used to evaluate the permeability of the mould upon the addition of fibres. The results obtained indicated that for the MOR test, the green (dewaxed) system has the highest MOR values than the fired and green (undewaxed) systems. The fired system is shown to have lowest MOR values among the three systems. For the permeability test, as expected. the fired system fibre addition specimens have higher permeability value than the green system. 2009-12 Thesis NonPeerReviewed application/pdf en http://eprints.utm.my/id/eprint/12221/6/SohWenHannMFKM2009.pdf Soh, Wen Hann (2009) Effect of oil palm fibre addition on the mechanical properties of shell mould investment casting. Masters thesis, Universiti Teknologi Malaysia, Faculty of Mechanical Engineering.
institution Universiti Teknologi Malaysia
building UTM Library
collection Institutional Repository
continent Asia
country Malaysia
content_provider Universiti Teknologi Malaysia
content_source UTM Institutional Repository
url_provider http://eprints.utm.my/
language English
topic TJ Mechanical engineering and machinery
TS Manufactures
spellingShingle TJ Mechanical engineering and machinery
TS Manufactures
Soh, Wen Hann
Effect of oil palm fibre addition on the mechanical properties of shell mould investment casting
description This research is aimed to investigate the effect of addition of organic fibre on the mechanical properties of the investment casting ceramic mould based on different length of fibres in the investment. Modulus of rupture (MOR) and permeability of the ceramic mould are evaluated. The MOR test contains three systems: green (undewaxed), green (dewaxed) and fired. The permeability test contains two systems: green (dewaxed) and fired. For the variation of fibre length, 3mm, 5mm, 7mm, 9mm are established. In each system, the MOR and permeability are compared between the fibre addition specimens and the non fibre addition specimen. Oil palm empty fruit bunch fibre is used as the additive in the investments. Colloidal silica and zircon sand are used to produce the ceramic mould. Firing temperature used is 700ºC. MOR three point bending testing machine is used to evaluate the strength of the mould. Permeability tester is used to evaluate the permeability of the mould upon the addition of fibres. The results obtained indicated that for the MOR test, the green (dewaxed) system has the highest MOR values than the fired and green (undewaxed) systems. The fired system is shown to have lowest MOR values among the three systems. For the permeability test, as expected. the fired system fibre addition specimens have higher permeability value than the green system.
format Thesis
author Soh, Wen Hann
author_facet Soh, Wen Hann
author_sort Soh, Wen Hann
title Effect of oil palm fibre addition on the mechanical properties of shell mould investment casting
title_short Effect of oil palm fibre addition on the mechanical properties of shell mould investment casting
title_full Effect of oil palm fibre addition on the mechanical properties of shell mould investment casting
title_fullStr Effect of oil palm fibre addition on the mechanical properties of shell mould investment casting
title_full_unstemmed Effect of oil palm fibre addition on the mechanical properties of shell mould investment casting
title_sort effect of oil palm fibre addition on the mechanical properties of shell mould investment casting
publishDate 2009
url http://eprints.utm.my/id/eprint/12221/6/SohWenHannMFKM2009.pdf
http://eprints.utm.my/id/eprint/12221/
_version_ 1643645893002395648
score 13.209306