Effect Of La2O3 Addition On The Hardness And Indentation Fracture Resistance Of Zta-Ceo2-La2o3 Ceramics

The effect of La2O3 addition to zirconia toughened alumina (ZTA) ceramics has been studied. CeO2 has been added in the ZTA system which acts as sintering additive. ZTA-CeO2 composition mixed with La2O3 weight percentage from 0.1 wt.% by weight to 10 wt.% . The compositions for each type of composit...

Full description

Saved in:
Bibliographic Details
Main Author: Rosli, Abdul Fatah Zulkarnain
Format: Monograph
Language:English
Published: Universiti Sains Malaysia 2018
Subjects:
Online Access:http://eprints.usm.my/53044/1/Effect%20Of%20La2O3%20Addition%20On%20The%20Hardness%20And%20Indentation%20Fracture%20Resistance%20Of%20Zta-Ceo2-La2o3%20Ceramics_Abdul%20Fatah%20Zulkarnain%20Rosli_B1_2018.pdf
http://eprints.usm.my/53044/
Tags: Add Tag
No Tags, Be the first to tag this record!
id my.usm.eprints.53044
record_format eprints
spelling my.usm.eprints.53044 http://eprints.usm.my/53044/ Effect Of La2O3 Addition On The Hardness And Indentation Fracture Resistance Of Zta-Ceo2-La2o3 Ceramics Rosli, Abdul Fatah Zulkarnain T Technology TN Mining Engineering. Metallurgy The effect of La2O3 addition to zirconia toughened alumina (ZTA) ceramics has been studied. CeO2 has been added in the ZTA system which acts as sintering additive. ZTA-CeO2 composition mixed with La2O3 weight percentage from 0.1 wt.% by weight to 10 wt.% . The compositions for each type of composition have been mixed, dried for 24 hours in the oven at 100 °C. This mixture is then compressed using hydraulic compressor in the mold cylinder at 10 MPa to form sample pellets. Next, this ZTA sample is sintered at 1600 °C with 4 hours soaking in a pressureless sintering furnace. Each of the sample was tested with a Vickers indentation of 30 kgf equivalent to 294 N. The Vickers indentation is intended to measure the hardness of the Vickers value and indentation fracture resistance for each sample. From the optimisation, ceramic sample ZTA-CeO2 with 0.85 wt.% La2O3 addition showed the highest Vickers hardness result with 1760.28 HV. ZTA ceramic samples with 1 wt.% addition of La2O3 showed the highest indentation fracture resistance results with 8.28 KIFR. Based on the SEM results, microstructure showed that the amount of the grain is increase with the increase of weight percentage of La2O3 addition in the ZTA system. The presence of the secondary phase of the elongated rod-like grains formed was known as LaAl11O18. This secondary phase plays an important role in increasing the value of hardness. Universiti Sains Malaysia 2018-06-01 Monograph NonPeerReviewed application/pdf en http://eprints.usm.my/53044/1/Effect%20Of%20La2O3%20Addition%20On%20The%20Hardness%20And%20Indentation%20Fracture%20Resistance%20Of%20Zta-Ceo2-La2o3%20Ceramics_Abdul%20Fatah%20Zulkarnain%20Rosli_B1_2018.pdf Rosli, Abdul Fatah Zulkarnain (2018) Effect Of La2O3 Addition On The Hardness And Indentation Fracture Resistance Of Zta-Ceo2-La2o3 Ceramics. Project Report. Universiti Sains Malaysia, Pusat Pengajian Kejuruteraan Bahan dan Sumber Mineral. (Submitted)
institution Universiti Sains Malaysia
building Hamzah Sendut Library
collection Institutional Repository
continent Asia
country Malaysia
content_provider Universiti Sains Malaysia
content_source USM Institutional Repository
url_provider http://eprints.usm.my/
language English
topic T Technology
TN Mining Engineering. Metallurgy
spellingShingle T Technology
TN Mining Engineering. Metallurgy
Rosli, Abdul Fatah Zulkarnain
Effect Of La2O3 Addition On The Hardness And Indentation Fracture Resistance Of Zta-Ceo2-La2o3 Ceramics
description The effect of La2O3 addition to zirconia toughened alumina (ZTA) ceramics has been studied. CeO2 has been added in the ZTA system which acts as sintering additive. ZTA-CeO2 composition mixed with La2O3 weight percentage from 0.1 wt.% by weight to 10 wt.% . The compositions for each type of composition have been mixed, dried for 24 hours in the oven at 100 °C. This mixture is then compressed using hydraulic compressor in the mold cylinder at 10 MPa to form sample pellets. Next, this ZTA sample is sintered at 1600 °C with 4 hours soaking in a pressureless sintering furnace. Each of the sample was tested with a Vickers indentation of 30 kgf equivalent to 294 N. The Vickers indentation is intended to measure the hardness of the Vickers value and indentation fracture resistance for each sample. From the optimisation, ceramic sample ZTA-CeO2 with 0.85 wt.% La2O3 addition showed the highest Vickers hardness result with 1760.28 HV. ZTA ceramic samples with 1 wt.% addition of La2O3 showed the highest indentation fracture resistance results with 8.28 KIFR. Based on the SEM results, microstructure showed that the amount of the grain is increase with the increase of weight percentage of La2O3 addition in the ZTA system. The presence of the secondary phase of the elongated rod-like grains formed was known as LaAl11O18. This secondary phase plays an important role in increasing the value of hardness.
format Monograph
author Rosli, Abdul Fatah Zulkarnain
author_facet Rosli, Abdul Fatah Zulkarnain
author_sort Rosli, Abdul Fatah Zulkarnain
title Effect Of La2O3 Addition On The Hardness And Indentation Fracture Resistance Of Zta-Ceo2-La2o3 Ceramics
title_short Effect Of La2O3 Addition On The Hardness And Indentation Fracture Resistance Of Zta-Ceo2-La2o3 Ceramics
title_full Effect Of La2O3 Addition On The Hardness And Indentation Fracture Resistance Of Zta-Ceo2-La2o3 Ceramics
title_fullStr Effect Of La2O3 Addition On The Hardness And Indentation Fracture Resistance Of Zta-Ceo2-La2o3 Ceramics
title_full_unstemmed Effect Of La2O3 Addition On The Hardness And Indentation Fracture Resistance Of Zta-Ceo2-La2o3 Ceramics
title_sort effect of la2o3 addition on the hardness and indentation fracture resistance of zta-ceo2-la2o3 ceramics
publisher Universiti Sains Malaysia
publishDate 2018
url http://eprints.usm.my/53044/1/Effect%20Of%20La2O3%20Addition%20On%20The%20Hardness%20And%20Indentation%20Fracture%20Resistance%20Of%20Zta-Ceo2-La2o3%20Ceramics_Abdul%20Fatah%20Zulkarnain%20Rosli_B1_2018.pdf
http://eprints.usm.my/53044/
_version_ 1736834795205296128
score 13.160551