Concentration effect of Zinc Acetate dihydrate as precursor in preparing Zinc Selenide through hydrothermal method

Zinc Selenide has been synthesized through hydrothermal method using Zinc Acetate Dihydrate (Zn(O2CCH3)2(H2O)2) and Se powder as the precursor. In a typical synthesis, Zn2+ and Se2- ion have been prepared separately and charged into a teflon-lined stainless steel autoclave. The ZnSe are characterize...

Full description

Saved in:
Bibliographic Details
Main Authors: Lee, Han Kee, Ashari, Fakhrurrazi, Talib, Zainal Abidin, Yap, Wing Fen, Ahmad Kamarudin, Mazliana, Effendi, N., Liew, Josephine Ying Chyi
Format: Article
Language:English
Published: National Institute of Research and Development of Materials Physics 2018
Online Access:http://psasir.upm.edu.my/id/eprint/72093/1/Concentration%20effect%20of%20Zinc%20Acetate%20dihydrate%20as%20precursor%20in%20preparing%20Zinc%20Selenide%20through%20hydrothermal%20method.pdf
http://psasir.upm.edu.my/id/eprint/72093/
http://www.chalcogen.ro/index.php/journals/chalcogenide-letters/11-cl/464-volume-15-number-10-october-2018
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:Zinc Selenide has been synthesized through hydrothermal method using Zinc Acetate Dihydrate (Zn(O2CCH3)2(H2O)2) and Se powder as the precursor. In a typical synthesis, Zn2+ and Se2- ion have been prepared separately and charged into a teflon-lined stainless steel autoclave. The ZnSe are characterized by X-ray diffraction (XRD), Field Emission Microscopy (FESEM), ultraviolet–visible spectroscopy (UV-Vis) and photoluminescence (PL). From the Pure ZnSe with main XRD peak at 2θ = 27.29°, 45.30°, 53.62°, 65.88°, 72.68° has been synthesized with the optical band gap energy (Eg) of 2.50 eV with emission peak at 486 nm.