FTIR and TGA analysis of biodegradable poly(lactic acid)/ treated kenaf bast fibre: effect of plasticizers
A biodegradable composite (PLA/KBF blends) was prepared using melt blending technique in a brabender mixer and characterized with FTIR and TGA analyzer. Five percent of triacetin and glycerol contents were used as plasticizers to plasticise PLA matrix. KBF was treated with 4% NaOH solution, whil...
Saved in:
Main Authors: | Othman, Maizatulnisa, Ibrahim, Nor Azowa, Wan Yunus, Wan Md. Zin, Abdan, Khalina, Khalid, Khalisanni |
---|---|
Format: | Article |
Language: | English |
Published: |
Universiti Putra Malaysia Press
2013
|
Online Access: | http://psasir.upm.edu.my/id/eprint/30411/1/31.%20FTIR%20and%20TGA%20Analysis%20of%20Biodegradable%20Poly.pdf http://psasir.upm.edu.my/id/eprint/30411/ http://pertanika.upm.edu.my/Pertanika%20PAPERS/JST%20Vol.%2021%20(1)%20Jan.%202013/14.%20Page%20151-160.pdf |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
FTIR and TGA analysis of biodegradable poly(lactic acid)/treated kenaf bast fibre: Effect of plasticizers
by: Maizatulnisa, Othman, et al.
Published: (2014) -
FTIR and TGA analysis of biodegradable poly(lactic acid)/treated kenaf bast fibre: effect of plasticizers
by: Othman, Maizatulnisa, et al.
Published: (2013) -
Poly(Lactic Acid)(PLA)-reinforced kenaf bast fiber composites : the effect of triacetin.
by: Ibrahim, Nor Azowa, et al.
Published: (2010) -
Effect of chemical surface treatment on
the mechanical properties of reinforced
plasticized poly(lactic acid) biodegradable
composites
by: Ibrahim, Nor Azowa, et al.
Published: (2011) -
Poly(Lactic Acid) (PLA)-reinforced
Kenaf Bast Fiber Composites:
The Effect of Triacetin
by: Othman, Maizatulnisa
Published: (2010)