Milling time and BPR dependance on permeability and losses of Ni0.5Zn0.5Fe2O4 synthesized via mechanical alloying process.

Ni0.5Zn0.5Fe2O4 has been synthesized using mechanical alloying method with two variables (milling time and ball-to-powder weight ratio (BPR)) were varied in order to study its effect on the magnetic properties of the material. The effects of these two variables were studied using XRD, SEM, TEM and l...

Full description

Saved in:
Bibliographic Details
Main Authors: Ismail, Ismayadi, Hashim , Mansor, Matori, Khamirul Amin, Alias, Rosidah, Hassan, Jumiah
Format: Article
Language:English
English
Published: Elsevier 2011
Online Access:http://psasir.upm.edu.my/id/eprint/25105/1/Milling%20time%20and%20BPR%20dependance%20on%20permeability%20and%20losses%20of%20Ni0.pdf
http://psasir.upm.edu.my/id/eprint/25105/
http://www.elsevier.com/
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:Ni0.5Zn0.5Fe2O4 has been synthesized using mechanical alloying method with two variables (milling time and ball-to-powder weight ratio (BPR)) were varied in order to study its effect on the magnetic properties of the material. The effects of these two variables were studied using XRD, SEM, TEM and later by impedance analyzer with the frequency range from 1 MHz to 1.8 GHz. The results obtained however show that there are no significant trends to relate the milling time and BPR with the permeability and losses of the material studied. After being sintered at 1150 °C, all the effects of alloying process seem to diminish.