Effect of a two-step solution heat treatment on the microstructure and mechanical properties of 332 aluminium silicon cast alloy
This paper investigated the effect of a two-step solution heat treatment on the mechanical properties and silicon-rich phase of 332 aluminium alloy. Traditional single-step T6 solution treatment (495 °C/6 h) increased the hardness value of the alloy by 5.96%, increased the tensile strength by 20.42%...
Saved in:
Main Authors: | Mohamed Ariff, Azmah Hanim, Chang, S. Chuan, Chuan, O. Khang |
---|---|
Format: | Article |
Language: | English |
Published: |
Elsevier
2011
|
Online Access: | http://psasir.upm.edu.my/id/eprint/22946/1/Effect%20of%20a%20two-step%20solution%20heat%20treatment%20on%20the%20microstructure%20and%20mechanical%20properties%20of%20332%20aluminium%20silicon%20cast%20alloy.pdf http://psasir.upm.edu.my/id/eprint/22946/ http://www.sciencedirect.com/science/article/pii/S0261306910007685 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Investigation mechanical properties and microstructure of aluminium silicon alloy using sand casting
by: Wong, Yin Ying
Published: (2010) -
Lost foam casting of aluminium - silicon (LM6) cast alloy
by: G. Khalifa, Alsalihin
Published: (2009) -
Effect of silicon on strength and fracture surfaces of aluminium–silicon casting and heat treated alloys
by: Haque, Md. Mohafizul, et al.
Published: (2006) -
Investigation on tool wear rate for modified and unmodified aluminium-silicon casting alloy
by: Haque, Md. Mohafizul, et al.
Published: (2009) -
Effect of quartz-silicon dioxide particulate on tensile properties of aluminium alloy cast composites
by: M. Sayuti, et al.
Published: (2011)