Enhanced critical current densities in MgB2 by mixing relatively impure boron powders.
Polycrystalline MgB2 samples were prepared from 99.98% purity Mg powder and different mixtures of relatively impure boron (99% pure crystalline boron and 95–97% amorphous boron) precursor powders. At both 6 and 20 K, for the mixed boron samples a doubling in Jc was observed over the highest values f...