The structural, mechanical, and biological variation of silica bioglasses obtained by different sintering temperatures
The challenges of forming a crystalline phase within 45S5 Bioglass® (45% SiO2-24.5% CaO-24.5% Na2O-6% P2O5 mol%) and its subsequent influence on the bioactivity of the bioglass were studied in this research. Bioglasses were sintered at 1400, 750, and 550 °C, using both melting and sol-gel methods. T...
Saved in:
Main Authors: | Sarmast Sh, M., Dayang Radiah, A. B., Hoey, D. A., Abdullah, N. |
---|---|
Format: | Article |
Published: |
Springer
2024
|
Online Access: | http://psasir.upm.edu.my/id/eprint/114507/ https://link.springer.com/article/10.1007/s10971-024-06480-z?error=cookies_not_supported&code=23ec5d94-87e3-44d3-b622-3f7213ce7fdc |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Evaluation of bioactivity and antibacterial properties of bioglass fabricated using a cellulose nano fibre template
by: Sarmast Shoushtari, Maryam, et al.
Published: (2023) -
Spark plasma sintered hydroxyapatite / bioglass composite for improved biological performance / Muhammad Rizwan
by: Muhammad , Rizwan
Published: (2019) -
Effect of calcination temperature on structure of mesoporous borosilicate bioglass
by: Md. Zain, S. K., et al.
Published: (2021) -
Low pressure spark plasma sintered hydroxyapatite and Bioglass® composite scaffolds for bone tissue repair
by: Rizwan, Muhammad, et al.
Published: (2018) -
Synthesis of bioactive glass using cellulose nano fibre template
by: Sh, M. Sarmast, et al.
Published: (2022)