Alloyability of warm formed FeCrAl powder compacts

Alloyability of warm formed Fe-based powder compacts is presented here. Iron (Fe) powder ASC100.29 was mixed with other alloying elements, namely chromium (Cr), and aluminum (Al) powder for 60. min and compacted at 150. °C by applying 130. kN axial loading, simultaneously from upper and lower punche...