A way to limit the long-term degradation of solid oxide fuel cell cathode by decorating the surface with K2NiF4-Structure Pr4Ni3O10+� phase

Prolonged annealing of La0.6Sr0.4Co0.2Fe0.8O3-� (LSCF) at 700 �C for 1000 h resulted in phase segregation on the surface in the form of submicron-sized SrO on the grains and micron-sized CoFe2O4 particles near the grain boundaries during electrical conductivity relaxation (ECR) measurements. The pre...