EPRB423 Project II Electrical properties of Bi-2212 and Ti added Bi-2212 superconductors
Bismuth based Bi-2212 phase and Ti added Bi-2212 phase high temperature superconductors are prepared using solid-state reaction method. Transport critical current, Ic was measured at 77 K by using the standard four point probes and compared. The addition of Ti in bismuth based Bi-2212 phase signific...
Saved in:
Main Author: | |
---|---|
Format: | text::Thesis |
Language: | English |
Published: |
2023
|
Subjects: | |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
id |
my.uniten.dspace-20930 |
---|---|
record_format |
dspace |
spelling |
my.uniten.dspace-209302023-05-05T08:06:10Z EPRB423 Project II Electrical properties of Bi-2212 and Ti added Bi-2212 superconductors Shahril Bin Abu Bakar Polycrystalline semiconductors Superconductors Bismuth based Bi-2212 phase and Ti added Bi-2212 phase high temperature superconductors are prepared using solid-state reaction method. Transport critical current, Ic was measured at 77 K by using the standard four point probes and compared. The addition of Ti in bismuth based Bi-2212 phase significantly influenced Ic. Ti added Bi-2212 bulk sample is better than pure Bi-2212 bulk sample by having a higher value of Ic. The result suggested that the Ti added Bi-2212 sample has better physical property and higher critical current density compared with the pure Bi-2212 sample. 2023-05-03T15:35:49Z 2023-05-03T15:35:49Z 2003 Resource Types::text::Thesis https://irepository.uniten.edu.my/handle/123456789/20930 en application/pdf |
institution |
Universiti Tenaga Nasional |
building |
UNITEN Library |
collection |
Institutional Repository |
continent |
Asia |
country |
Malaysia |
content_provider |
Universiti Tenaga Nasional |
content_source |
UNITEN Institutional Repository |
url_provider |
http://dspace.uniten.edu.my/ |
language |
English |
topic |
Polycrystalline semiconductors Superconductors |
spellingShingle |
Polycrystalline semiconductors Superconductors Shahril Bin Abu Bakar EPRB423 Project II Electrical properties of Bi-2212 and Ti added Bi-2212 superconductors |
description |
Bismuth based Bi-2212 phase and Ti added Bi-2212 phase high temperature superconductors are prepared using solid-state reaction method. Transport critical current, Ic was measured at 77 K by using the standard four point probes and compared. The addition of Ti in bismuth based Bi-2212 phase significantly influenced Ic. Ti added Bi-2212 bulk sample is better than pure Bi-2212 bulk sample by having a higher value of Ic. The result suggested that the Ti added Bi-2212 sample has better physical property and higher critical current density compared with the pure Bi-2212 sample. |
format |
Resource Types::text::Thesis |
author |
Shahril Bin Abu Bakar |
author_facet |
Shahril Bin Abu Bakar |
author_sort |
Shahril Bin Abu Bakar |
title |
EPRB423 Project II Electrical properties of Bi-2212 and Ti added Bi-2212 superconductors |
title_short |
EPRB423 Project II Electrical properties of Bi-2212 and Ti added Bi-2212 superconductors |
title_full |
EPRB423 Project II Electrical properties of Bi-2212 and Ti added Bi-2212 superconductors |
title_fullStr |
EPRB423 Project II Electrical properties of Bi-2212 and Ti added Bi-2212 superconductors |
title_full_unstemmed |
EPRB423 Project II Electrical properties of Bi-2212 and Ti added Bi-2212 superconductors |
title_sort |
eprb423 project ii electrical properties of bi-2212 and ti added bi-2212 superconductors |
publishDate |
2023 |
_version_ |
1806427832372428800 |
score |
13.211869 |