High temperature corrosion behaviour of steel with a Carbonate deposit at 1123K
The high temperature corrosion behavior of A1S1 304 austenitic stainless steel and S45C carbon steel were studied in presence with CaCO3 salt at 1123K for 24,48,72, 96 and 120 hour. The studies were carried out to determine the mass change vs times, the morphological structures of deposits on the su...
Saved in:
Main Authors: | Habsah, Md Ishak, Mohammed Misbahul, Amin, Nazree, Derman, Khairul Rafezi, Ahmad |
---|---|
Format: | Article |
Language: | English |
Published: |
School of Materials Engineering
2009
|
Subjects: | |
Online Access: | http://dspace.unimap.edu.my/xmlui/handle/123456789/6151 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Effect of Inhibitors on the Corrosion of AISI-1018 Steel in Sea-Water Environment
by: Mohammed Misbahul, Amin, et al.
Published: (2008) -
The effectiveness of Sodium Benzoate as corrosion inhibitor for stainless steel in seawater environment
by: H. B., Senin, et al.
Published: (2009) -
High temperature corrosion behaviour of austenitic stainless steel with CaCO₃ and MgCO₃ deposit
by: Habsah, Md Ishak
Published: (2014) -
Hot corrosion behaviour of Austenitic Steel-308 in Chloride salts
by: Mohammed Misbahul, Amin, et al.
Published: (2009) -
Corrosion properties of Stainless steel
by: Abang Fairol, Abang Sarbini
Published: (2009)