The interlaminar shear strength test of helical wound glass fibre reinforced epoxy laminates subjected to hydrothermal ageing
Link to publisher's homepage at http://www.ttp.net/
Saved in:
Main Authors: | , , , , , |
---|---|
Other Authors: | |
Format: | Article |
Language: | English |
Published: |
Trans Tech Publications
2014
|
Subjects: | |
Online Access: | http://dspace.unimap.edu.my:80/dspace/handle/123456789/35120 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
id |
my.unimap-35120 |
---|---|
record_format |
dspace |
spelling |
my.unimap-351202014-06-05T08:20:37Z The interlaminar shear strength test of helical wound glass fibre reinforced epoxy laminates subjected to hydrothermal ageing Mohd Shukry, Abdul Majid, Dr. Mohd Afendi, Rojan, Dr. Ruslizam, Daud, Dr. Nasrul Amri, Mohd Amin, Dr. Azizul, Mohamad M. Hekman shukry@unimap.edu.my afendirojan@unimap.edu.my ruslizam@unimap.edu.my nasrulamri.mohdamin@unimap.edu.my azizul@unimap.edu.my Interlaminar shear strength test Hydrothermal Glass fibre reinforced epoxy Composite laminates Link to publisher's homepage at http://www.ttp.net/ This paper presents the experimental investigation of interlaminar shear strength (ILSS) tests of helical wound glass fibre reinforced epoxy (GRE) pipes subjected to hydrothermal ageing. Currently, the test is being used by composite pipes manufacturers as the alternative internal quality monitoring program for detection of manufacturing changes and reconfirmation of the design basis of composite pipes. The test specimens were cut in hoop direction from helically wound GRE composite pipes after exposure of 0, 250, 500, 1000-hour water at 80°C. The ILSS tests of the GRE samples were then conducted in accordance with ASTM D2344, and the results were analyzed to evaluate the durability performance of the laminates. The results show a clear degradation in the bonding strength between fibres and resin system interface after 500-1000-hour water exposure at 80°C. This findings show a good agreement in the trend observed with the standard qualification procedure elucidated in ASTM D2992 standard. Hence, ILSS test shows a great potential to be used as the internal short-term mechanical test method to qualify a new resin, curing agent or glass fibre in accordance to the next approach. 2014-06-05T08:20:37Z 2014-06-05T08:20:37Z 2014-06 Article Applied Mechanics and Materials, vol. 554, 2014, pages 391-395 1660-9336 http://www.scientific.net/AMM.554.391 http://dspace.unimap.edu.my:80/dspace/handle/123456789/35120 10.4028/www.scientific.net/AMM.554.391 en Trans Tech Publications |
institution |
Universiti Malaysia Perlis |
building |
UniMAP Library |
collection |
Institutional Repository |
continent |
Asia |
country |
Malaysia |
content_provider |
Universiti Malaysia Perlis |
content_source |
UniMAP Library Digital Repository |
url_provider |
http://dspace.unimap.edu.my/ |
language |
English |
topic |
Interlaminar shear strength test Hydrothermal Glass fibre reinforced epoxy Composite laminates |
spellingShingle |
Interlaminar shear strength test Hydrothermal Glass fibre reinforced epoxy Composite laminates Mohd Shukry, Abdul Majid, Dr. Mohd Afendi, Rojan, Dr. Ruslizam, Daud, Dr. Nasrul Amri, Mohd Amin, Dr. Azizul, Mohamad M. Hekman The interlaminar shear strength test of helical wound glass fibre reinforced epoxy laminates subjected to hydrothermal ageing |
description |
Link to publisher's homepage at http://www.ttp.net/ |
author2 |
shukry@unimap.edu.my |
author_facet |
shukry@unimap.edu.my Mohd Shukry, Abdul Majid, Dr. Mohd Afendi, Rojan, Dr. Ruslizam, Daud, Dr. Nasrul Amri, Mohd Amin, Dr. Azizul, Mohamad M. Hekman |
format |
Article |
author |
Mohd Shukry, Abdul Majid, Dr. Mohd Afendi, Rojan, Dr. Ruslizam, Daud, Dr. Nasrul Amri, Mohd Amin, Dr. Azizul, Mohamad M. Hekman |
author_sort |
Mohd Shukry, Abdul Majid, Dr. |
title |
The interlaminar shear strength test of helical wound glass fibre reinforced epoxy laminates subjected to hydrothermal ageing |
title_short |
The interlaminar shear strength test of helical wound glass fibre reinforced epoxy laminates subjected to hydrothermal ageing |
title_full |
The interlaminar shear strength test of helical wound glass fibre reinforced epoxy laminates subjected to hydrothermal ageing |
title_fullStr |
The interlaminar shear strength test of helical wound glass fibre reinforced epoxy laminates subjected to hydrothermal ageing |
title_full_unstemmed |
The interlaminar shear strength test of helical wound glass fibre reinforced epoxy laminates subjected to hydrothermal ageing |
title_sort |
interlaminar shear strength test of helical wound glass fibre reinforced epoxy laminates subjected to hydrothermal ageing |
publisher |
Trans Tech Publications |
publishDate |
2014 |
url |
http://dspace.unimap.edu.my:80/dspace/handle/123456789/35120 |
_version_ |
1643797712459530240 |
score |
13.222552 |