The effect of sintering temperature on mechanical properties of natural and synthetic Hydroxyapatite with Alumina (1%) as an additive

A multi sintering temperature of hydroxyapatite (HA) will give an affect not only for the shape, composition and arrangement of the microstructure, but also to a high impact on mechanical properties of those samples. Natural and synthetic HA adding with Alumina separately, will change a mechanical p...

Full description

Saved in:
Bibliographic Details
Main Author: Rozaima Yusoff
Other Authors: Sri Asliza Md Amin (Advisor)
Format: Learning Object
Language:English
Published: Universiti Malaysia Perlis 2008
Subjects:
Online Access:http://dspace.unimap.edu.my/xmlui/handle/123456789/3376
Tags: Add Tag
No Tags, Be the first to tag this record!
id my.unimap-3376
record_format dspace
spelling my.unimap-33762008-11-28T04:05:46Z The effect of sintering temperature on mechanical properties of natural and synthetic Hydroxyapatite with Alumina (1%) as an additive Rozaima Yusoff Sri Asliza Md Amin (Advisor) Sintering Sinter (Metallurgy) Materials engineering Hydroxyapatite -- Thermal analysis Biomedical materials Aluminum oxide A multi sintering temperature of hydroxyapatite (HA) will give an affect not only for the shape, composition and arrangement of the microstructure, but also to a high impact on mechanical properties of those samples. Natural and synthetic HA adding with Alumina separately, will change a mechanical properties of pure HA to make it suitable apply to many medical application nowadays. A using of natural HA will go through with a heat treatment of cow bone to remove an impurities and protein to avoid it affected a properties of final samples. It’s different by using a synthetic HA, where this powder is then mix with alumina as an additive, PEG as a binder and Calgon as anti-agglomerate. Both type of HA will prepare using a wet method and roll the mixing on the ball milling for 16 hours. Mixing is then dry in oven for 3 hours and crush also sieve to get fine particles. Granulation is spraying on bulk mixing for 8-10% before it compact with 50MPa using un-axial load. A dense sample is dry in oven and after sinter at 1150oC and 1200oC before it will test their density and porosity, flexural test (MOR), X-ray diffraction (XRD) and scanning electron microscopic (SEM). TGA/DTA and also Malvern Mastersizer analysis is done to measure a characterization of materials before sinter. From both HA used, synthetic HA will give a higher density and strength when it sinter at higher temperature. 2008-11-28T04:05:46Z 2008-11-28T04:05:46Z 2008-05 Learning Object http://hdl.handle.net/123456789/3376 en Universiti Malaysia Perlis School of Materials Engineering
institution Universiti Malaysia Perlis
building UniMAP Library
collection Institutional Repository
continent Asia
country Malaysia
content_provider Universiti Malaysia Perlis
content_source UniMAP Library Digital Repository
url_provider http://dspace.unimap.edu.my/
language English
topic Sintering
Sinter (Metallurgy)
Materials engineering
Hydroxyapatite -- Thermal analysis
Biomedical materials
Aluminum oxide
spellingShingle Sintering
Sinter (Metallurgy)
Materials engineering
Hydroxyapatite -- Thermal analysis
Biomedical materials
Aluminum oxide
Rozaima Yusoff
The effect of sintering temperature on mechanical properties of natural and synthetic Hydroxyapatite with Alumina (1%) as an additive
description A multi sintering temperature of hydroxyapatite (HA) will give an affect not only for the shape, composition and arrangement of the microstructure, but also to a high impact on mechanical properties of those samples. Natural and synthetic HA adding with Alumina separately, will change a mechanical properties of pure HA to make it suitable apply to many medical application nowadays. A using of natural HA will go through with a heat treatment of cow bone to remove an impurities and protein to avoid it affected a properties of final samples. It’s different by using a synthetic HA, where this powder is then mix with alumina as an additive, PEG as a binder and Calgon as anti-agglomerate. Both type of HA will prepare using a wet method and roll the mixing on the ball milling for 16 hours. Mixing is then dry in oven for 3 hours and crush also sieve to get fine particles. Granulation is spraying on bulk mixing for 8-10% before it compact with 50MPa using un-axial load. A dense sample is dry in oven and after sinter at 1150oC and 1200oC before it will test their density and porosity, flexural test (MOR), X-ray diffraction (XRD) and scanning electron microscopic (SEM). TGA/DTA and also Malvern Mastersizer analysis is done to measure a characterization of materials before sinter. From both HA used, synthetic HA will give a higher density and strength when it sinter at higher temperature.
author2 Sri Asliza Md Amin (Advisor)
author_facet Sri Asliza Md Amin (Advisor)
Rozaima Yusoff
format Learning Object
author Rozaima Yusoff
author_sort Rozaima Yusoff
title The effect of sintering temperature on mechanical properties of natural and synthetic Hydroxyapatite with Alumina (1%) as an additive
title_short The effect of sintering temperature on mechanical properties of natural and synthetic Hydroxyapatite with Alumina (1%) as an additive
title_full The effect of sintering temperature on mechanical properties of natural and synthetic Hydroxyapatite with Alumina (1%) as an additive
title_fullStr The effect of sintering temperature on mechanical properties of natural and synthetic Hydroxyapatite with Alumina (1%) as an additive
title_full_unstemmed The effect of sintering temperature on mechanical properties of natural and synthetic Hydroxyapatite with Alumina (1%) as an additive
title_sort effect of sintering temperature on mechanical properties of natural and synthetic hydroxyapatite with alumina (1%) as an additive
publisher Universiti Malaysia Perlis
publishDate 2008
url http://dspace.unimap.edu.my/xmlui/handle/123456789/3376
_version_ 1643787820175720448
score 13.214268