Preparation, characterization and properties of polypropylene/waste tire dust (PP/WTD)
Thermoplastics and waste rubber from scrap tires were mixed to prepare polypropylene/waste tire dust (PPIWTD) blends. All blends were prepared in an internal mixer at a temperature of 180°C, a rotor speed of 50 rpm and a mixing period between 9 and 13 min. Characterization was done to determine the...
Saved in:
Main Author: | |
---|---|
Format: | Thesis |
Language: | English |
Published: |
Pulau Pinang: Universiti Sains Malaysia
2014
|
Subjects: | |
Online Access: | http://dspace.psnz.umt.edu.my/xmlui/handle/123456789/2758 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Summary: | Thermoplastics and waste rubber from scrap tires were mixed to prepare polypropylene/waste tire dust (PPIWTD) blends. All blends were prepared in an
internal mixer at a temperature of 180°C, a rotor speed of 50 rpm and a mixing period between 9 and 13 min. Characterization was done to determine the
properties of the blends and to investigate the effects of WTD size, application of dynamic vulcanization and co-agents, addition of other polymeric materials and a 6-month exposure to natural weathering on the mechanical properties, morphology, swelling resistance and thermal properties of the blends. |
---|