Investigation on weld quality using different filler metals

Dissimilar welding process yields unwanted disadvantages on the weld joint due to the large difference between stainless steel-aluminium sheets melting points and nearly zeros solid solubility between these two metals. Aluminium AA6061 and stainless steel SUS304 were lap-welded by using Metal Inert...

Full description

Saved in:
Bibliographic Details
Main Author: Zetty Akhtar, Abd Malek
Format: Undergraduates Project Papers
Language:English
Published: 2012
Subjects:
Online Access:http://umpir.ump.edu.my/id/eprint/4903/1/cd7357_66.pdf
http://umpir.ump.edu.my/id/eprint/4903/
Tags: Add Tag
No Tags, Be the first to tag this record!
id my.ump.umpir.4903
record_format eprints
spelling my.ump.umpir.49032021-06-04T04:47:33Z http://umpir.ump.edu.my/id/eprint/4903/ Investigation on weld quality using different filler metals Zetty Akhtar, Abd Malek TA Engineering (General). Civil engineering (General) Dissimilar welding process yields unwanted disadvantages on the weld joint due to the large difference between stainless steel-aluminium sheets melting points and nearly zeros solid solubility between these two metals. Aluminium AA6061 and stainless steel SUS304 were lap-welded by using Metal Inert Gas (MIG) welding with aluminium filler ER5356 and stainless steel filler ER308LSi. The effect of welding voltage and type of filler metals used to the weld joints were studied. The welding voltage had significance effect to the welding process, as high voltage resulted in poor appearance of the weld joint. Joints between aluminium and stainless steel using aluminium filler have good microstructure as it shows enrichment of eutectic silicon particle, thus increase the hardness of the joint. The intermetallic compound layer occur between heat affected zone and fusion zone. The hardness value of welded seam in this joint range from 60 to 100 HV. The fracture in tensile test occurred at the edge of the joint before derive into welded seam with the highest tensile strength of 104.4 MPa. Meanwhile, aluminium-stainless steel joints using stainless steel filler contains carbide precipitate in its microstructure, which is undesirable in welding process. The enrichment of chromium particles indicates that there is element addition in weld joint throughout welding process. The hardness value of the welded seam range from 180 to 230 HV and the highest tensile strength is 61.76 MPa. Based on this study, it can be concluded that aluminium filler ER5356 is the optimum filler in joining dissimilar metal aluminium AA6061 and stainless steel SUS 304. 2012-06 Undergraduates Project Papers NonPeerReviewed application/pdf en http://umpir.ump.edu.my/id/eprint/4903/1/cd7357_66.pdf Zetty Akhtar, Abd Malek (2012) Investigation on weld quality using different filler metals. Faculty of Mechanical Engineering, Universiti Malaysia Pahang.
institution Universiti Malaysia Pahang
building UMP Library
collection Institutional Repository
continent Asia
country Malaysia
content_provider Universiti Malaysia Pahang
content_source UMP Institutional Repository
url_provider http://umpir.ump.edu.my/
language English
topic TA Engineering (General). Civil engineering (General)
spellingShingle TA Engineering (General). Civil engineering (General)
Zetty Akhtar, Abd Malek
Investigation on weld quality using different filler metals
description Dissimilar welding process yields unwanted disadvantages on the weld joint due to the large difference between stainless steel-aluminium sheets melting points and nearly zeros solid solubility between these two metals. Aluminium AA6061 and stainless steel SUS304 were lap-welded by using Metal Inert Gas (MIG) welding with aluminium filler ER5356 and stainless steel filler ER308LSi. The effect of welding voltage and type of filler metals used to the weld joints were studied. The welding voltage had significance effect to the welding process, as high voltage resulted in poor appearance of the weld joint. Joints between aluminium and stainless steel using aluminium filler have good microstructure as it shows enrichment of eutectic silicon particle, thus increase the hardness of the joint. The intermetallic compound layer occur between heat affected zone and fusion zone. The hardness value of welded seam in this joint range from 60 to 100 HV. The fracture in tensile test occurred at the edge of the joint before derive into welded seam with the highest tensile strength of 104.4 MPa. Meanwhile, aluminium-stainless steel joints using stainless steel filler contains carbide precipitate in its microstructure, which is undesirable in welding process. The enrichment of chromium particles indicates that there is element addition in weld joint throughout welding process. The hardness value of the welded seam range from 180 to 230 HV and the highest tensile strength is 61.76 MPa. Based on this study, it can be concluded that aluminium filler ER5356 is the optimum filler in joining dissimilar metal aluminium AA6061 and stainless steel SUS 304.
format Undergraduates Project Papers
author Zetty Akhtar, Abd Malek
author_facet Zetty Akhtar, Abd Malek
author_sort Zetty Akhtar, Abd Malek
title Investigation on weld quality using different filler metals
title_short Investigation on weld quality using different filler metals
title_full Investigation on weld quality using different filler metals
title_fullStr Investigation on weld quality using different filler metals
title_full_unstemmed Investigation on weld quality using different filler metals
title_sort investigation on weld quality using different filler metals
publishDate 2012
url http://umpir.ump.edu.my/id/eprint/4903/1/cd7357_66.pdf
http://umpir.ump.edu.my/id/eprint/4903/
_version_ 1702170033894981632
score 13.159267