Rubberwood Fiber Treatment by Laccase Enzyme and Its Application in Medium Density Fiberboard
In this work physico-chemical properties of rubber wood fiber were analyzed after laccase treatment and evaluated the performance of medium density fiberboard (MDF) fabricated from the treated fiber. In a single parameter study, two different times i.e. 60 min and 120 min of laccase treatment were a...
Saved in:
Main Authors: | , , , , , |
---|---|
Format: | Article |
Language: | English |
Published: |
Oriental Scientific Pub Co
2015
|
Subjects: | |
Online Access: | http://umpir.ump.edu.my/id/eprint/12714/1/fkksa-2015-arun-Rubberwood%20Fiber%20Treatment%20by%20Laccase.pdf http://umpir.ump.edu.my/id/eprint/12714/ http://microbiologyjournal.org/jmabsread.php?snoid=2801&month=Sep&year=2015 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
id |
my.ump.umpir.12714 |
---|---|
record_format |
eprints |
spelling |
my.ump.umpir.127142018-03-07T03:11:46Z http://umpir.ump.edu.my/id/eprint/12714/ Rubberwood Fiber Treatment by Laccase Enzyme and Its Application in Medium Density Fiberboard Mohammed, Nasir Othman, Sulaiman Rokiah, Hashim Hossain, Kaizar Gupta, Arun Mohd, Asim TP Chemical technology In this work physico-chemical properties of rubber wood fiber were analyzed after laccase treatment and evaluated the performance of medium density fiberboard (MDF) fabricated from the treated fiber. In a single parameter study, two different times i.e. 60 min and 120 min of laccase treatment were applied at constant temperature, enzyme concentration and pH. After the pulp treatment, fibers were sieved out and transferred in to autoclave at 121 °C for 15 min to stop further enzyme reaction. Treated fiber was dried in electric oven drier at 80-90°C for 24 hr to dry up the fiber until constant moisture content. Crystallinity index of the fiber was measured by X-ray diffraction method and it was observed maximum up to 14% higher compared to untreated fiber. The treated fiber was further analyzed for FE-SEM, TGA and compared with untreated fiber in order to evaluate its properties. Fiber treated with enzyme exhibited superiority in fiber surface structure and thermal degradation over untreated fibers. The MDF prepared from improved crystalline fiber showed improved physical and mechanical properties as compared to the MDF from untreated fiber. Oriental Scientific Pub Co 2015 Article PeerReviewed application/pdf en http://umpir.ump.edu.my/id/eprint/12714/1/fkksa-2015-arun-Rubberwood%20Fiber%20Treatment%20by%20Laccase.pdf Mohammed, Nasir and Othman, Sulaiman and Rokiah, Hashim and Hossain, Kaizar and Gupta, Arun and Mohd, Asim (2015) Rubberwood Fiber Treatment by Laccase Enzyme and Its Application in Medium Density Fiberboard. Journal of Pure and Applied Microbiology, 9 (3). pp. 2095-2100. ISSN 0973-7510 http://microbiologyjournal.org/jmabsread.php?snoid=2801&month=Sep&year=2015 |
institution |
Universiti Malaysia Pahang |
building |
UMP Library |
collection |
Institutional Repository |
continent |
Asia |
country |
Malaysia |
content_provider |
Universiti Malaysia Pahang |
content_source |
UMP Institutional Repository |
url_provider |
http://umpir.ump.edu.my/ |
language |
English |
topic |
TP Chemical technology |
spellingShingle |
TP Chemical technology Mohammed, Nasir Othman, Sulaiman Rokiah, Hashim Hossain, Kaizar Gupta, Arun Mohd, Asim Rubberwood Fiber Treatment by Laccase Enzyme and Its Application in Medium Density Fiberboard |
description |
In this work physico-chemical properties of rubber wood fiber were analyzed after laccase treatment and evaluated the performance of medium density fiberboard (MDF) fabricated from the treated fiber. In a single parameter study, two different times i.e. 60 min and 120 min of laccase treatment were applied at constant temperature, enzyme concentration and pH. After the pulp treatment, fibers were sieved out and transferred in to autoclave at 121 °C for 15 min to stop further enzyme reaction. Treated fiber was dried in electric oven drier at 80-90°C for 24 hr to dry up the fiber until constant moisture content. Crystallinity index of the fiber was measured by X-ray diffraction method and it was observed maximum up to 14% higher compared to untreated fiber. The treated fiber was further analyzed for FE-SEM, TGA and compared with untreated fiber in order to evaluate its properties. Fiber treated with enzyme exhibited superiority in fiber surface structure and thermal degradation over untreated fibers. The MDF prepared from improved crystalline fiber showed improved physical and mechanical properties as compared to the MDF from untreated fiber. |
format |
Article |
author |
Mohammed, Nasir Othman, Sulaiman Rokiah, Hashim Hossain, Kaizar Gupta, Arun Mohd, Asim |
author_facet |
Mohammed, Nasir Othman, Sulaiman Rokiah, Hashim Hossain, Kaizar Gupta, Arun Mohd, Asim |
author_sort |
Mohammed, Nasir |
title |
Rubberwood Fiber Treatment by Laccase Enzyme and Its Application in Medium Density Fiberboard |
title_short |
Rubberwood Fiber Treatment by Laccase Enzyme and Its Application in Medium Density Fiberboard |
title_full |
Rubberwood Fiber Treatment by Laccase Enzyme and Its Application in Medium Density Fiberboard |
title_fullStr |
Rubberwood Fiber Treatment by Laccase Enzyme and Its Application in Medium Density Fiberboard |
title_full_unstemmed |
Rubberwood Fiber Treatment by Laccase Enzyme and Its Application in Medium Density Fiberboard |
title_sort |
rubberwood fiber treatment by laccase enzyme and its application in medium density fiberboard |
publisher |
Oriental Scientific Pub Co |
publishDate |
2015 |
url |
http://umpir.ump.edu.my/id/eprint/12714/1/fkksa-2015-arun-Rubberwood%20Fiber%20Treatment%20by%20Laccase.pdf http://umpir.ump.edu.my/id/eprint/12714/ http://microbiologyjournal.org/jmabsread.php?snoid=2801&month=Sep&year=2015 |
_version_ |
1643666975540379648 |
score |
13.209306 |