Effect of sintering temperatures on sr-doped NiO ceramics
Sr - doped NiO ceramic was prepared using solid state method. The calcination temperature used at 950 oC for 4 hours and the sintering temperatures was varied from 1100 to 1300 oC for 3 hours. The results depict the microstructures increasing in grains size (1-8 μm) by increase of sintering temperat...