Study of delayed cracking behaviors of hydrogen-charged SUS304L deep drawn cylindrical cups under elevated blank holding forces / Mohd Shahir Hadzir
In this paper the effect of hydrogen charged SUS304L deep drawn cylindrical cups under elevated blank holding forces are investigated. A round SUS 304L blanks was deep drawn at 8, 9, 10 and 11 kN blank holding force, BHF using a die, after the specimens were hydrogen charged for 6, 12, and 24 hours...