Thermal activation of ordinary Portland cement-slag mortars

Thirty one mix proportions of ordinary Portland cement (OPC)-slag mortars (OSM) used to study the effects of temperature on early and ultimate strengths. Three levels of slag (0, 40, and 50) and different temperatures were used; it was found that 50 is the optimum level and 60°C with 20. h duration...