Fiber length, thermal, mechanical, and dynamic mechanical properties of injection-molded glass-fiber/polyamide 6,6: Plasticization effect

Unreinforced- and glass fiber-reinforced-polyamide 6,6 specimens were subjected to dry, 50 RH, and wet conditions. FLD study showed that more fiber degradation occurred during processing of the composites with higher fiber loading. TGA results revealed that about 2 and 5 levels of moisture have been...

Full description

Saved in:
Bibliographic Details
Main Authors: Hassan, A., Salleh, N.M., Yahya, R., Sheikh, M.R.K.
Format: Article
Published: 2011
Subjects: