Reactions of Palm Oil-Based mcl-PHAs with Epoxidized Natural Rubber
A palm oil-based medium-chain-length polyhydroxyalkanoate (mcl-PHA) was allowed to react with epoxidized natural rubber (ENR). There was no noticeable reaction at ambient temperature for short reaction times. However, after 30 min at 170 degrees C, the mcl-PHA underwent thermal degradation to genera...
Saved in:
Main Authors: | Lee, S.Y., Hassan, A., Tan, I.K.P., Terakawa, K., Ichikawa, N., Gan, S.N. |
---|---|
Format: | Article |
Published: |
Wiley
2010
|
Subjects: | |
Online Access: | http://eprints.um.edu.my/5415/ |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Recovery of Medium-Chain-Length Polyhydroxyalkanoates (PHAs) Through Enzymatic Digestion Treatments and Ultrafiltration
by: Yasotha, K., et al.
Published: (2006) -
Chemical characterization of medium-chain-length polyhydroxyalkanoates (PHAs) recovered by enzymatic treatment and ultrafiltration
by: Kathiraser, Y., et al.
Published: (2007) -
Kinetics of Thermodegradation of Palm Kernel Oil Derived Medium-Chain-Length Polyhydroxyalkanoates
by: Sin, M.C., et al.
Published: (2012) -
Characterization of oligomeric hydroxyalkanoic acids from thermal decomposition of palm kernel oil-based biopolyester
by: Sin, M.C., et al.
Published: (2011) -
Degradation of medium-chain-length polyhydroxyalkanoates in tropical forest and mangrove soils
by: Lim, S.P., et al.
Published: (2005)