The use of pro-degradant additive (PDA) to enhance the oxidative degradability of polymers has been successful in hydrocarbon plastics, but few, if any studies have been conducted to evaluate the effect of PDA on natural rubbers. This study investigated thermal, and photo oxidative degradation of na...