Effect of sintering holding time on low-temperature degradation of yttria stabilised zirconia ceramics

Effect of sintering holding time on low-temperature degradation of 3 mol-% yttria stabilised zirconia was investigated. Yttria stabilised zirconia samples were sintered using a two-step sintering cycle. The samples were initially heated to 1500°C with the heating rate of 10°C min−1, held for 1 minut...

Full description

Saved in:
Bibliographic Details
Main Authors: Sutharsini, U., Ramesh, S., Wong, Y.H., Misran, H., Yusuf, F., Tan, C.Y., Purbolaksono, J., Teng, W.D.
Format: Article
Published: Maney Publishing 2014
Subjects:
Online Access:http://eprints.um.edu.my/13009/
http://www.maneyonline.com/doi/abs/10.1179/1432891714Z.000000000988?journalCode=mri
http://dx.doi.org/10.1179/1432891714Z.000000000988