The optical effect of porous silicon doped nano-silver particles / Mohammad Zaifah Ahmad
Porous Silicon (PSi) has been formed by anodically etching p-type Si [100] wafer in hydrofluoric (HF) solution at 1:1 ratio of ethanol. The samples were prepared at various etching time which is at 5 minutes, 10 minutes, 15 minutes and 20 minutes, that will give different percentage of porosity. The...