Sintered strength of ti-6Al-4V by metal injection molding (MIM) using palm stearin binder / N. H. Mohamad Nor...[et al.]
Metal injection molding (MIM) is a metal working process used to compact Titanium, Ti-6Al-4V and the binder through injection moulding process. In this work, Titanium Ti-6Al-4V was mixed with palm stearin (PS) and polyethylene (PE) which act as a binder. Palm stearin (PS) is a potential binder syste...
Saved in:
Main Authors: | N. H., Mohamad Nor, M. H., Ismail, H., Husain, J. B., Saedon, M., Newishy |
---|---|
Format: | Article |
Language: | English |
Published: |
Faculty of Mechanical Engineering Universiti Teknologi MARA (UiTM)
2019
|
Subjects: | |
Online Access: | http://ir.uitm.edu.my/id/eprint/36350/1/36350.pdf http://ir.uitm.edu.my/id/eprint/36350/ https://jmeche.uitm.edu.my/ |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Development of porous Ti-6Al-4V mix with palm stearin
binder by metal injection molding technique
by: Jamaludin, Mohamad Ikhwan, et al.
Published: (2015) -
Characterisation of stainless steel 316L and palm stearin based binder by using metal injection molding (MIM) process
by: Musa Zainal Abidin, Murni Farahin
Published: (2014) -
Parameter optimization of injection molding Ti-6Al-4V powder and palm stearin binder system for highest green density using Taguchi method
by: Jamaludin, Khairur Rijal, et al.
Published: (2010) -
Optimization of injection molding parameter of ti-6al-4v powder mix with palm stearin and polyethylene for the highest green strength by using taguchi method
by: M. Nor, N. H., et al.
Published: (2011) -
Parameter optimization of debinding injection moulded Ti-6Al-4V mix
with palm stearin and polyethylene
by: Jamaludin, M. I., et al.
Published: (2014)