Electrochemical characterization of graphene-based nanocomposites as transducer material for highly sensitive biosensors was performed. Parameters that were varied include graphene oxide (GO) concentration and amount of added gold nanoparticles (AuNPs) as well as Nafion as binder for enhancing elect...
Saved in:
Main Authors: | , |
---|---|
Format: | Conference or Workshop Item |
Language: | English |
Published: |
IIUM
2016
|
Subjects: | |
Online Access: | http://irep.iium.edu.my/52690/8/52690-edited.pdf http://irep.iium.edu.my/52690/ |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
id |
my.iium.irep.52690 |
---|---|
record_format |
dspace |
spelling |
my.iium.irep.526902016-11-29T07:12:31Z http://irep.iium.edu.my/52690/ Electrochemical characterization of Graphene-based transducers for biosensor development Arris, Farrah Aida Wan Salim, Wan Wardatul Amani T Technology (General) Electrochemical characterization of graphene-based nanocomposites as transducer material for highly sensitive biosensors was performed. Parameters that were varied include graphene oxide (GO) concentration and amount of added gold nanoparticles (AuNPs) as well as Nafion as binder for enhancing electrical conductivity of the transducer layer. The nanocomposite-modified GCE transducer layers were fabricated via a simple two-step drop-cast and subsequent electrochemical reduction. Cyclic voltammetry (CV) was used to characterize the redox capability of the transducer layer. Electrochemical deposition of ultra-highly-concentrated single-layer graphene oxide (UHC GO) suspension with a concentration of 6.2 mg/ml gave higher anodic peak current, Ipa, after electrochemical reduction compared to most peak currents reported in the literature for a 3-mm inner-diameter electrode; adding UHC GO:AuNPs in a 2:1 ratio followed by electrochemical reduction resulted in even higher Ipa, whereas adding UHC GO:Nafion in a 4:1 ratio gave promising results for prolonged shelf-life of the biosensor. Therefore, UHC GO-AuNPs-Nafion as nanocomposite is an excellent precursor for the development of a redox-active transducer that results in highly sensitive biosensors. IIUM 2016 Conference or Workshop Item REM application/pdf en http://irep.iium.edu.my/52690/8/52690-edited.pdf Arris, Farrah Aida and Wan Salim, Wan Wardatul Amani (2016) Electrochemical characterization of Graphene-based transducers for biosensor development. In: 4th International Conference on Biotechnology Engineering 2016 (ICBioE 2016), 25th-27th July 2016, Kuala Lumpur. |
institution |
Universiti Islam Antarabangsa Malaysia |
building |
IIUM Library |
collection |
Institutional Repository |
continent |
Asia |
country |
Malaysia |
content_provider |
International Islamic University Malaysia |
content_source |
IIUM Repository (IREP) |
url_provider |
http://irep.iium.edu.my/ |
language |
English |
topic |
T Technology (General) |
spellingShingle |
T Technology (General) Arris, Farrah Aida Wan Salim, Wan Wardatul Amani Electrochemical characterization of Graphene-based transducers for biosensor development |
description |
Electrochemical characterization of graphene-based nanocomposites as transducer material for highly sensitive biosensors was performed. Parameters that were varied include graphene oxide (GO) concentration and amount of added gold nanoparticles (AuNPs) as well as Nafion as binder for enhancing electrical conductivity of the transducer layer. The nanocomposite-modified GCE transducer layers were fabricated via a simple two-step drop-cast and subsequent electrochemical reduction. Cyclic voltammetry (CV) was used to characterize the redox capability of the transducer layer. Electrochemical deposition of ultra-highly-concentrated single-layer graphene oxide (UHC GO) suspension with a concentration of 6.2 mg/ml gave higher anodic peak current, Ipa, after electrochemical reduction compared to most peak currents reported in the literature for a 3-mm inner-diameter electrode; adding UHC GO:AuNPs in a 2:1 ratio followed by
electrochemical reduction resulted in even higher Ipa, whereas adding UHC GO:Nafion in a 4:1 ratio gave
promising results for prolonged shelf-life of the biosensor. Therefore, UHC GO-AuNPs-Nafion as nanocomposite is an excellent precursor for the development of a redox-active transducer that results in
highly sensitive biosensors. |
format |
Conference or Workshop Item |
author |
Arris, Farrah Aida Wan Salim, Wan Wardatul Amani |
author_facet |
Arris, Farrah Aida Wan Salim, Wan Wardatul Amani |
author_sort |
Arris, Farrah Aida |
title |
Electrochemical characterization of Graphene-based transducers for biosensor development |
title_short |
Electrochemical characterization of Graphene-based transducers for biosensor development |
title_full |
Electrochemical characterization of Graphene-based transducers for biosensor development |
title_fullStr |
Electrochemical characterization of Graphene-based transducers for biosensor development |
title_full_unstemmed |
Electrochemical characterization of Graphene-based transducers for biosensor development |
title_sort |
electrochemical characterization of graphene-based transducers for biosensor development |
publisher |
IIUM |
publishDate |
2016 |
url |
http://irep.iium.edu.my/52690/8/52690-edited.pdf http://irep.iium.edu.my/52690/ |
_version_ |
1643614211860856832 |
score |
13.211869 |