Effect of sintering on the physical and mechanical properties of Co-Cr-Mo (F-75)/HAP composites

This paper reports on the effects of HAP addition and sintering temperature on the microstructure and properties of the F-75/HAP composites fabricated by powder metallurgy. Co-Cr-Mo (F-75) is used in orthopedics because of its excellent biocompatibility when implanted to human or animal body. Hydrox...

Full description

Saved in:
Bibliographic Details
Main Authors: Nur Maizatul Shima Adzali,, Shamsul Baharin Jamaludin,, Mohd Nazree Derman,
Format: Article
Language:English
Published: Universiti Kebangsaan Malaysia 2013
Online Access:http://journalarticle.ukm.my/6687/1/11_Nur_Maizatul_Shima.pdf
http://journalarticle.ukm.my/6687/
http://www.ukm.my/jsm/
Tags: Add Tag
No Tags, Be the first to tag this record!
id my-ukm.journal.6687
record_format eprints
spelling my-ukm.journal.66872016-12-14T06:41:55Z http://journalarticle.ukm.my/6687/ Effect of sintering on the physical and mechanical properties of Co-Cr-Mo (F-75)/HAP composites Nur Maizatul Shima Adzali, Shamsul Baharin Jamaludin, Mohd Nazree Derman, This paper reports on the effects of HAP addition and sintering temperature on the microstructure and properties of the F-75/HAP composites fabricated by powder metallurgy. Co-Cr-Mo (F-75) is used in orthopedics because of its excellent biocompatibility when implanted to human or animal body. Hydroxyapatite (HAP) powders have been used as fillers because HAP is the one of the most effective biocompatible materials with similarities to mineral constituents of bones and teeth. HAP powders (chemical formula Ca10(PO4)6 (OH)2) have been added to Co-Cr-Mo alloys in composition of 0 to 10 wt. %. The mixtures were then milled, cold compacted at 550 MPa, before sintered at 1100 and 1200°C in a tube furnace. The density, porosity, microhardness and compressive strength were measured. The composites that have been sintered at temperature 1200°C showed better physical and mechanical properties than those produced at 1100°C. After sintering at 1200°C, the samples show higher density, compared with the sample sintered at 1100°C. The sample with no HAP which have been sintered at 1200°C has the highest microhardness (208.9 HV), compared with the same sample sintered at 1100°C (194.3HV). As the temperature is increased from 1100 to 1200°C, the value of compressive strength increased from 184.538 to 341.086 MPa. Microstructural analysis for line scan showed that, as the sintering temperature was increased, there was good interface bonding between HAP particles and matrix F-75. Universiti Kebangsaan Malaysia 2013-12 Article PeerReviewed application/pdf en http://journalarticle.ukm.my/6687/1/11_Nur_Maizatul_Shima.pdf Nur Maizatul Shima Adzali, and Shamsul Baharin Jamaludin, and Mohd Nazree Derman, (2013) Effect of sintering on the physical and mechanical properties of Co-Cr-Mo (F-75)/HAP composites. Sains Malaysiana, 42 (12). pp. 1763-1768. ISSN 0126-6039 http://www.ukm.my/jsm/
institution Universiti Kebangsaan Malaysia
building Perpustakaan Tun Sri Lanang Library
collection Institutional Repository
continent Asia
country Malaysia
content_provider Universiti Kebangsaan Malaysia
content_source UKM Journal Article Repository
url_provider http://journalarticle.ukm.my/
language English
description This paper reports on the effects of HAP addition and sintering temperature on the microstructure and properties of the F-75/HAP composites fabricated by powder metallurgy. Co-Cr-Mo (F-75) is used in orthopedics because of its excellent biocompatibility when implanted to human or animal body. Hydroxyapatite (HAP) powders have been used as fillers because HAP is the one of the most effective biocompatible materials with similarities to mineral constituents of bones and teeth. HAP powders (chemical formula Ca10(PO4)6 (OH)2) have been added to Co-Cr-Mo alloys in composition of 0 to 10 wt. %. The mixtures were then milled, cold compacted at 550 MPa, before sintered at 1100 and 1200°C in a tube furnace. The density, porosity, microhardness and compressive strength were measured. The composites that have been sintered at temperature 1200°C showed better physical and mechanical properties than those produced at 1100°C. After sintering at 1200°C, the samples show higher density, compared with the sample sintered at 1100°C. The sample with no HAP which have been sintered at 1200°C has the highest microhardness (208.9 HV), compared with the same sample sintered at 1100°C (194.3HV). As the temperature is increased from 1100 to 1200°C, the value of compressive strength increased from 184.538 to 341.086 MPa. Microstructural analysis for line scan showed that, as the sintering temperature was increased, there was good interface bonding between HAP particles and matrix F-75.
format Article
author Nur Maizatul Shima Adzali,
Shamsul Baharin Jamaludin,
Mohd Nazree Derman,
spellingShingle Nur Maizatul Shima Adzali,
Shamsul Baharin Jamaludin,
Mohd Nazree Derman,
Effect of sintering on the physical and mechanical properties of Co-Cr-Mo (F-75)/HAP composites
author_facet Nur Maizatul Shima Adzali,
Shamsul Baharin Jamaludin,
Mohd Nazree Derman,
author_sort Nur Maizatul Shima Adzali,
title Effect of sintering on the physical and mechanical properties of Co-Cr-Mo (F-75)/HAP composites
title_short Effect of sintering on the physical and mechanical properties of Co-Cr-Mo (F-75)/HAP composites
title_full Effect of sintering on the physical and mechanical properties of Co-Cr-Mo (F-75)/HAP composites
title_fullStr Effect of sintering on the physical and mechanical properties of Co-Cr-Mo (F-75)/HAP composites
title_full_unstemmed Effect of sintering on the physical and mechanical properties of Co-Cr-Mo (F-75)/HAP composites
title_sort effect of sintering on the physical and mechanical properties of co-cr-mo (f-75)/hap composites
publisher Universiti Kebangsaan Malaysia
publishDate 2013
url http://journalarticle.ukm.my/6687/1/11_Nur_Maizatul_Shima.pdf
http://journalarticle.ukm.my/6687/
http://www.ukm.my/jsm/
_version_ 1643736856719785984
score 13.18916