Volume shrinkage during carbothermic reduction of low-grade iron ore containing goethite and coal composite
The volume shrinkage and reduction behavior of low-grade iron ore goethite during the solid-state carbothermic process was studied and compared to synthetic goethite. The carbothermic reduction process using low-grade coal as a reducing agent was carried out in the temperature range 1000-1200 °C up...
Saved in:
Main Authors: | Setiawan, Agung, Ina Ermawati,, Anggraini, Farras, Abidin, Faizinal, Abdul Hapid,, Kawigraha, Adji, Harjanto, Sri, Rhamdhani, M. Akbar |
---|---|
Format: | Article |
Language: | English |
Published: |
Penerbit Universiti Kebangsaan Malaysia
2022
|
Online Access: | http://journalarticle.ukm.my/19484/1/20.pdf http://journalarticle.ukm.my/19484/ https://www.ukm.my/jsm/malay_journals/jilid51bil5_2022/KandunganJilid51Bil5_2022.html |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Carbothermic reaction characteristics of Indonesian Lateritic Nickel Ore
by: Sri Harjanto, et al.
Published: (2010) -
Mineralogical characterizations of Langkawi Ilmenite ore for carbothermal reduction
by: N. F. M., Yunos, et al.
Published: (2022) -
The Carbothermic Route to Magnesium
by: Hasan, Nurul
Published: (2006) -
Bioleaching of low grade refractory gold ore
by: Jaapar, Jefri
Published: (2001) -
Kinetic study of reduction roasting of mixed laterite ore and coal
by: -, Pramusanto, et al.
Published: (2011)