Failure investigation of natural gas pipeline
A study was carried out to investigate the probable cause or events that might have led to the failure of two parallel natural gas pipes, API 5L X42 carbon steel (NPS 8) and the SDR 17, 125 mm medium density polyethylene pipes. These two pipes were laid side by side in the same trench with a water p...
Saved in:
Main Authors: | Abdul Majid, Zulkifli, Mohsin, Rahmat |
---|---|
Format: | Article |
Published: |
Springer
2012
|
Subjects: | |
Online Access: | http://eprints.utm.my/id/eprint/33538/ http://dx.doi.org/10.1007/s13369-012-0236-z |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Failure analysis of natural gas pipeline
by: Abdul Majid, Zulkifli, et al.
Published: (2008) -
Water jetting impact on natural gas pipeline
by: Abdul Majid, Z., et al.
Published: (2008) -
Experimental and numerical investigation of high-pressure water jetting effect toward NPS8 natural gas pipeline integrity-establishing safety distance perimeter
by: Majid, Z. A., et al.
Published: (2015) -
Modeling Of Natural Gas Phase
Behaviour In Pipeline
by: Lee , Teik Hui
Published: (2009) -
Erosive wear of natural gas pipeline
by: Abdul Majid, Zulkifli, et al.
Published: (2008)