Evaluation on an internal surface crack in a compound tube

In this paper stress intensity factors of a longitudinal semiellipti-cal surface crack on the inner surface in a compound tube subjected to internal pressure are presented. Variations of modulus of elasticity and thickness for the inner part of the tube are used in order to evaluate their effects on...