Preparation of anti rust paint with waste expanded Polystyrene
A formula for making paint using waste expanded polystyrene foam (EPS) as a binder in place of alkyd resin in most of the commercial paint was developed. Through the experiment the formula follows: the base material (EPS) is 27%, the solvent 43% and the pigment 30%. The morphology and performance c...